Regeneration Method of Waste Lubricating Oil Containing Glue
A technology for waste lubricating oil and lubricating oil, applied in the field of lubricating oil, can solve problems such as inability to remove lubricating oil, inability to block impurities, and quality of kneading into rubber, so as to achieve improved quality of pretreated oil, short production cycle and low cost Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] according to figure 1 As shown, 1000kg of waste lubricating oil is extracted into a pretreatment reactor provided with a heater 7 (the top of the pretreatment reactor is provided with a fume collection device 3) by using waste oil pumping power equipment, heated and separated, and heated to 120°C, after heating for 30 minutes, keep the temperature constant, add adsorbent 4 high alumina attapulgite concentrate, the amount added is about 0.5% of the waste oil mass, stir for 15 minutes, so that the adsorbent 4 can fully absorb and polymerize the waste lubricating oil After the colloidal components in the mixture are fully adsorbed and combined, stop heating and keep the temperature above room temperature to stand for 5 hours, and the colloidal particles, carbon black, impurities, etc. will gather downward as much as possible (that is, the adsorbed heavy colloidal impurities 6) by pretreatment The lower port of the reactor is discharged to the sewage tank 1, the upper layer...
Embodiment 2
[0032]Pump 1,000kg of waste lubricating oil into the preprocessor, heat and separate, heat to 125°C, keep the temperature constant after heating for 50 minutes, add high-alumina attapulgite concentrate as an adsorbent, and the amount added is about 0.7% of the waste oil mass , stirred for 30 minutes, so that the adsorbent fully adsorbs and polymerizes the colloidal components in the waste lubricating oil. After fully adsorbing and combining, stop heating and keep the temperature above room temperature for 8 hours. After precipitation, the upper layer is pretreated lubricating oil , the pretreated lubricating oil is subjected to specific gravity separation, molecular sieves are added to the liquid obtained after separation for fine decomposition, and then the finely decomposed lubricating oil is sieved and filtered to obtain about 750 kg of finely purified lubricating oil. The oil content of the heavy rubber part in the lubricating oil after pretreatment is lower than 5%, and th...
Embodiment 3
[0034] Pump 1000kg of waste lubricating oil into the preprocessor, heat and separate, heat to 123°C, keep the temperature constant after heating for 40 minutes, add high-alumina attapulgite concentrate as an adsorbent, and the amount added is about 0.6% of the waste oil mass , stirred for 20 minutes to make the adsorbent fully absorb and polymerize the colloidal components in the waste lubricating oil. After fully adsorbing and combining, stop heating and keep the temperature above room temperature for 6.5 hours. After precipitation, the upper layer is pretreated lubricating oil , the pretreated lubricating oil is subjected to specific gravity separation, molecular sieves are added to the liquid obtained after separation for fine decomposition, and then the finely decomposed lubricating oil is sieved and filtered to obtain about 700 kg of finely purified lubricating oil. The oil content of the heavy rubber part in the lubricating oil after pretreatment is lower than 5%, and the...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 