An escape chute and semi-fixed technology, which is applied in life-saving equipment, building rescue, etc., can solve the problems such as the difficulty of fixing the escape chute system, and achieve the goals of improving anti-ultraviolet aging ability, smooth connection, improving stability and dispersion Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0079] The present invention is a semi-mobile and semi-fixed escape slide device with an anti-ultraviolet aging fiber-reinforced polymer-based composite material, which includes 2kg of compound anti-ultraviolet aging agent, 60kg of matrix resin, 30kg of reinforcing fiber, curing agent and accelerator Dosage 8kg.
[0080] In this embodiment, the components in the compound anti-ultraviolet aging agent are zinc oxide and UV-531, the weight ratio is 50:50, the matrix resin is epoxy resin, the reinforcing fiber is glass fiber, curing agent ethylenediamine, accelerator For, DMP-30.
[0081] The preparation steps of the above-mentioned anti-ultraviolet aging fiber-reinforced polymer-based composite material for the slideway are as follows:
[0082] 1) Disperse the inorganic particle ultraviolet absorber zinc oxide and organic ultraviolet absorber UV-531 in ethanol at a weight ratio of 50kg:50kg, mix uniformly, and dry.
[0083] 2) Mix the treated compound anti-ultraviolet aging age...
Embodiment 2
[0086] The present invention is a kind of anti-ultraviolet aging fiber-reinforced polymer-based composite material for the slide in the semi-mobile and semi-fixed escape chute device, including 5kg of compound anti-ultraviolet aging agent, 50kg of matrix resin, 40kg of reinforcing fiber, curing agent and accelerator dose 5kg.
[0087] In this example, the components of the compound anti-ultraviolet aging agent are titanium dioxide and UVP-327, the weight ratio is 80:20, the matrix resin is epoxy resin, the reinforcing fiber is boron fiber, and the curing agent is ethylenediamine and accelerator for K-54.
[0088] The preparation steps of the above-mentioned anti-ultraviolet aging fiber-reinforced polymer-based composite material for the slideway are as follows:
[0089] 1) The inorganic nanoparticle ultraviolet absorber titanium dioxide and the organic ultraviolet absorber UVP-327 are dispersed in ethanol at a weight ratio of 80:20, mixed uniformly, and dried.
[0090] 2) Mi...
Embodiment 3
[0093] The present invention is a kind of anti-ultraviolet aging fiber-reinforced polymer-based composite material for the slideway in the semi-mobile and semi-fixed escape chute device, which includes 1 kg of compound anti-ultraviolet aging agent, 70 kg of matrix resin, 20 kg of reinforcing fiber, curing agent and accelerator Dosage 10kg.
[0094]In this embodiment, the components of the compound anti-ultraviolet aging agent are carbon black and UV-P, the matrix resin is epoxy resin, the reinforcing fiber is glass fiber, the curing agent is phthalic anhydride and the accelerator is DMP-30.
[0095] The preparation steps of the above-mentioned anti-ultraviolet aging fiber-reinforced polymer-based composite material for the slideway are as follows:
[0096] 1) Disperse the inorganic nanoparticle ultraviolet absorber carbon black and the organic ultraviolet absorber UV-P in ethanol at a weight ratio of 40:60, mix uniformly, and dry.
[0097] 2) Mix the treated compound anti-ult...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com