Embodiment 1
[0036] Example 1 Emollient and moisturizing cream (I)
[0037] The formula is shown in Table 1.
[0038] Table 1
[0039]
[0040] The preparation method is as follows:
[0041] (1) Put component A into an oil pan and heat to 80°C, stir and mix evenly to dissolve completely, and set aside.
[0042] (2) Put component B into the emulsification pot and heat to 80°C, stir and mix evenly to dissolve completely, and set aside.
[0043] (3) Control the homogenization speed at 5000r / min and the stirring speed at 300r / min. Quickly put component A into the emulsification pot and homogenize for 15 minutes.
[0044] (4) Stop homogenization, keep the temperature at 80 degrees, stir at 400r / min, and stir for 10 minutes.
[0045] (5) Keep the stirring speed at 400r / min and cool down.
[0046] (6) Cool down to 40°C, add component C into the emulsification pot, vacuumize, and stir evenly.
[0047] (7) Stir evenly, cool down to 35°C, discharge, fill and seal.
Embodiment 2
[0048] Example 2 Emollient and moisturizing cream (Ⅱ)
[0049] The formula is shown in Table 2.
[0050] Table 2
[0051]
[0052] The preparation method is as follows:
[0053] (1) Put component A into an oil pan and heat to 80°C, stir and mix evenly to dissolve completely, and set aside.
[0054] (2) Put component B into the emulsification pot and heat to 80°C, stir and mix evenly to dissolve completely, and set aside.
[0055] (3) Control the homogenization speed at 5000r / min and the stirring speed at 300r / min. Quickly put component A into the emulsification pot and homogenize for 15 minutes.
[0056] (4) Stop homogenization, keep the temperature at 80 degrees, stir at 400r / min, and stir for 10 minutes.
[0057] (5) Keep the stirring speed at 400r / min and cool down.
[0058] (6) Cool down to 40°C, add component C into the emulsification pot, vacuumize, and stir evenly.
[0059] (7) Stir evenly, cool down to 35°C, discharge, fill and seal.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com