[0027] A technical method for increasing wicker color retention time, comprising the following steps:
[0028] (1) select straight wicker without bending and stuttering, polish and polish it, use 100 mesh sandpaper to polish for the first time in the process of polishing, eliminate burrs, and then send it into the polishing machine for polishing;
[0029] (2) prepare soaking liquid, calculate by mass parts, the following components hydrogen peroxide 60%, nonionic surfactant 3%, anionic surfactant 3%, softening agent 5%, boric acid 6%, fatty acid 10%, ethanol 15% and 10% thickening agent are uniformly mixed, stirred at a constant speed with a centrifugal mixer for 8 minutes, then sent to a heating furnace for heating, and stopped heating when the temperature rises to 90°C, and let it cool naturally, and pour it into a soaking tank after cooling Then put the polished wicker into the soaking box for soaking. The soaking solution is specially formulated for wicker. When the wicker...
Embodiment 2
[0038] A technical method for increasing wicker color retention time, comprising the following steps:
[0039] (1) select straight wicker without bending and stuttering, polish and polish it, use 100 mesh sandpaper to polish for the first time in the process of polishing, eliminate burrs, and then send it into the polishing machine for polishing;
[0040] (2) prepare soaking liquid, calculate by mass parts, the following components hydrogen peroxide 663%, nonionic surfactant 4%, anionic surfactant 4%, softening agent 6%, boric acid 8%, fatty acid 15%, ethanol After uniform mixing of 13% and 11% tackifier, use a centrifugal mixer to stir at a constant speed for 8 minutes, then send it to a heating furnace for heating, stop heating when the temperature rises to 90°C, let it cool naturally, and pour it into a soaking tank after cooling Then put the polished wicker into the soaking box for soaking. The soaking solution is specially formulated for wicker. When the wicker is complet...
Embodiment 3
[0049] A technical method for increasing wicker color retention time, comprising the following steps:
[0050] (1) select straight wicker without bending and stuttering, polish and polish it, use 100 mesh sandpaper to polish for the first time in the process of polishing, eliminate burrs, and then send it into the polishing machine for polishing;
[0051] (2) prepare soaking liquid, calculate by mass parts, the following components hydrogen peroxide 65%, nonionic surfactant 5%, anionic surfactant 5%, softening agent 8%, boric acid 10%, fatty acid 20%, ethanol 15% and 12% thickening agent are uniformly mixed, stirred at a constant speed with a centrifugal mixer for 8 minutes, then sent to a heating furnace for heating, and stopped heating when the temperature rises to 90°C, and let it cool naturally, and pour it into a soaking tank after cooling Then put the polished wicker into the soaking box for soaking. The soaking solution is specially formulated for wicker. When the wicke...