A technology for caring oil and furniture, applied in the direction of paint, polishing composition and coating containing biocide, it can solve the problems of cracking, unpleasant smell, damage and other problems of wood products, and achieves increased friction, good manual polishing, The effect of promoting penetration
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0046] A preparation method of solid wood furniture care oil, is characterized in that, comprises the steps:
[0047] Step 1, in parts by weight, weigh the following ingredients:
[0048] 10 parts corn oil,
[0049] 10 parts paraffin,
[0050] 12 parts soybeans,
[0051] 20 parts lanolin,
[0052] 8 parts saponins,
[0053] 7 parts of peony,
[0054] 6 parts aloe vera,
[0055] Sea buckthorn seed oil 7 parts,
[0056] 6 parts of glycerin,
[0057] 8 parts of perfluorinated wax,
[0058] 7 parts emulsifier,
[0059] Antifungal agent 0.4 part.
[0060] Step 2, heat the corn oil to 65°C with water, slowly add paraffin, and stir continuously with a stirring rod during the melting process of the paraffin; after fully heating and mixing, maintain the temperature at 72°C for 3 minutes, stop heating and wait for the mixture to cool to 45°C °C, forming a mixture a;
[0061] Step 3, the soybeans are ground, and the soybean liquid is obtained after filtering;
[0062] Step 4...
Embodiment 2
[0067] A preparation method of solid wood furniture care oil, is characterized in that, comprises the steps:
[0068] Step 1, in parts by weight, weigh the following ingredients:
[0069] 8 parts corn oil,
[0070] 12 parts paraffin,
[0071] 12 parts soybeans,
[0072] 22 parts lanolin,
[0073] 9 parts saponins,
[0074] 8 parts of peony,
[0075] 3 parts aloe vera,
[0076] Sea buckthorn seed oil 10 parts,
[0077] 6 parts of glycerin,
[0078] 8 parts of perfluorinated wax,
[0079] 7 parts emulsifier,
[0080] 0.6 part of antifungal agent.
[0081] Step 2, heat the corn oil to 68°C with water, slowly add paraffin, and stir continuously with a stirring rod during the melting process of the paraffin; after fully heating and mixing, maintain the temperature at 72°C for 3 minutes, stop heating and wait for the mixture to cool to 45°C °C, forming a mixture a;
[0082] Step 3, the soybeans are ground, and the soybean liquid is obtained after filtering;
[0083] Step ...
Embodiment 3
[0088] A preparation method of solid wood furniture care oil, is characterized in that, comprises the steps:
[0089] Step 1, in parts by weight, weigh the following ingredients:
[0090] 12 parts corn oil,
[0091] 16 parts of paraffin,
[0092] 8 servings of soybeans,
[0093] 23 parts lanolin,
[0094] 9 parts saponins,
[0095] 8 parts of peony,
[0096] Aloe vera 8 parts,
[0097] Sea buckthorn seed oil 12 parts,
[0098] 4 parts of glycerin,
[0099] 12 parts of perfluorinated wax,
[0100] 4 parts emulsifier,
[0101] 0.5 part of antifungal agent.
[0102] Step 2, heat the corn oil to 68°C with water, slowly add paraffin, and stir continuously with a stirring rod during the melting process of the paraffin; after fully heating and mixing, maintain the temperature at 72°C for 3 minutes, stop heating and wait for the mixture to cool to 45°C °C, forming a mixture a;
[0103] Step 3, the soybeans are ground, and the soybean liquid is obtained after filtering;
...