A moisture-proof and mortar technology, which is applied in the direction of stairs, treads, and ladder-like structures, can solve problems that affect the construction quality and pouring quality of prefabricated stairs, poor drying shrinkage volume stability, and expansion agents can’t play a role, etc., to solve shrinkage cracking Difficulty, stable construction performance and volume stability, effect of improving volume stability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0069] The present invention also proposes a preparation method of moisture-absorbing expansion grouting mortar, which comprises the following steps:
[0070] Weigh the raw materials according to the aforementioned materials and proportions of the moisture-proof expansion grouting mortar, and mix them uniformly to obtain the moisture-proof expansion grouting mortar, which is a dry-mix composition.
[0071] The present invention also proposes an application of the moisture-insulating expansion grouting mortar prepared according to the aforementioned method in field installation of adjustable step height prefabricated stairs.
[0072] Preferably, it includes the following steps: adding water to the dry mix composition, stirring, and pouring.
[0073] Preferably, in practical application of the above-mentioned absolute moisture expansion grouting mortar, 10-12% of the mass of water needs to be added and stirred by a mixer with a linear speed of 6-10 m / s for 3-5 minutes.
Embodiment 1~5
[0076] Weigh the raw materials according to the formula shown in Attached Table 1 and Attached Table 2, mix the various raw materials evenly, and add them to the mortar mixer together with water, wherein the weight of the added water accounts for 11.0% of the perfusion mortar dry mix composition, and the stirring blade The linear speed is 8m / s, and the rapid stirring is 4 minutes, and the moisture-absorbing grouting mortar with high fluidity, early strength and fast hardening, and no shrinkage can be obtained.
[0077] Among them, the mass percentage ratio of the three-stage gradation of quartz sand is 30.0% of 20-40 mesh quartz sand, 40.0% of 40-70 mesh quartz sand, and 30.0% of 70-120 mesh quartz sand.
[0078] According to GB / T 50448-2015 "Technical Specifications for Application of Cement-Based Grouting Materials", perform performance tests such as initial fluidity, 30min fluidity, 1d compressive strength, 3d compressive strength, 28d compressive strength and 24h vertical e...
PUM
Property | Measurement | Unit |
---|---|---|
specific surface area | aaaaa | aaaaa |
specific surface area | aaaaa | aaaaa |
specific surface area | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com