Tremolite jade laminated composite material and method for producing same
A composite material and production method technology, applied in the field of furniture, can solve the problems of no significant application of tremolite jade, lack of practical technology, etc., and achieve the effect of strengthening strength and processability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0033] In this embodiment, jasper from Canada is used as the tremolite jade thin plate. The jasper has a Mohs hardness of 6.0-6.5, contains iron, and its Mg 2+ / (Mg 2+ +Fe 2+ ) ratio is 0.973. The substrate used in this example is transparent tempered glass. The above-mentioned jasper from Canada was cut into jasper sheets with a thickness of 2.8 mm, and then compounded with transparent reinforced glass through a transparent adhesive to obtain the attached figure 1 The translucent tremolite jade laminated composite material shown can be used as a light-transmitting plate.
Embodiment 2
[0035] The tremolite jade thin plate used in this embodiment is the same as that of Example 1, and is jasper from Canada. The jasper has a Mohs hardness of 6.0-6.5, contains iron, and its Mg 2+ / (Mg 2+ +Fe 2+ ) ratio is 0.971. The thickness of the jasper sheet used in this embodiment is 2.5 millimeters, the first substrate used is an aluminum honeycomb material, the second substrate is a wooden board, and through the compounding of an adhesive, the attached figure 2 The tremolite jade laminate composite is shown. The surface of the tremolite jade laminated composite material is a tremolite jade thin plate, and the bottom surface is a wooden material, which can be used as a material for furniture.
Embodiment 3
[0037] The tremolite jade sheet used in this example is jasper from Russia. Like the jasper from Canada, the jasper from Siberia, Russia has a Mohs hardness of 6.0-6.5, contains iron, and its Mg 2+ / (Mg 2+ +Fe 2+ ) ratio is 0.976. The thickness of the jasper in this embodiment is 2.5 millimeters, by compounding with the first substrate aluminum plate and the second substrate aluminum honeycomb under the action of adhesive, the attached image 3 The tremolite jade laminated composite material shown can be used as a building material or a decorative material.
PUM
Property | Measurement | Unit |
---|---|---|
Thickness | aaaaa | aaaaa |
Thickness | aaaaa | aaaaa |
Area | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com