Preparation method and application of electroactive ionic liquid-based mesoporous silicon modified electrode
A technology of ionic liquid and modified electrode, which is applied in the field of electrochemical enzyme-free sensor preparation, can solve the problem of unclear chemical reaction mechanism between ferricyanide ion and hydrogen peroxide, etc., achieve simple and effective modification of electrode, and realize the effect of catalytic reduction
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] A method for preparing an electroactive ionic liquid-based mesoporous silicon modified electrode, the specific implementation steps are as follows:
[0030] a. Prepare 1.5 mg / mL ionic liquid modified mesoporous silicon solid particle (MCF-IL) dispersion and 2% polyvinyl alcohol solution by mass fraction;
[0031] b. Take the ionic liquid modified mesoporous silicon solid particle dispersion prepared in step a and mix it with the above polyvinyl alcohol solution. After mixing, the concentration of the mesoporous silicon solid particle dispersion is 1.5mg / mL, and the polyvinyl alcohol solution The mass fraction is 0.5‰, and the mixed solution is evenly mixed by vortex to make a drop coating solution;
[0032] c. Dispensing electrode: Vortex the dispensing solution prepared in step b, take 5 μL of the dispensing solution on the glassy carbon electrode, and dry overnight;
[0033] d.MCF-IL-Fe(CN) 6 3- / Preparation of PVA modified electrode
[0034] Put the glassy carbo...
Embodiment 2
[0040] A method for preparing an electroactive ionic liquid-based mesoporous silicon modified electrode, the specific implementation steps are as follows:
[0041] a. Prepare 2.0 mg / mL ionic liquid modified mesoporous silicon solid particle (MCF-IL) dispersion and 3.0% polyvinyl alcohol solution by mass fraction;
[0042] b. Take the ionic liquid modified mesoporous silicon solid particle dispersion prepared in step a and mix it with the above polyvinyl alcohol solution. After mixing, the concentration of the mesoporous silicon solid particle dispersion is 1.9mg / mL, and the polyvinyl alcohol solution The mass fraction is 1‰, and the mixed solution is evenly mixed by vortex to make a drop coating solution;
[0043] c. Dispensing electrode: Vortex the dispensing solution prepared in step b, take 8 μL of the dispensing solution on the glassy carbon electrode, and dry overnight;
[0044] d.MCF-IL-Fe(CN) 6 3- / Preparation of PVA modified electrode
[0045] Put the glassy carbo...
Embodiment 3
[0049] A method for preparing an electroactive ionic liquid-based mesoporous silicon modified electrode, the specific implementation steps are as follows:
[0050] a. Prepare 1.5 mg / mL ionic liquid modified mesoporous silicon solid particle (MCF-IL) dispersion and 2% polyvinyl alcohol solution by mass fraction;
[0051] b. Take the ionic liquid modified mesoporous silicon solid particle dispersion prepared in step a and mix it with the above polyvinyl alcohol solution. After mixing, the concentration of the mesoporous silicon solid particle dispersion is 0.95mg / mL, and the polyvinyl alcohol solution The mass fraction is 0.5‰, and the mixed solution is evenly mixed by vortex to make a drop coating solution;
[0052] c. Dispensing electrode: Vortex the dispensing solution prepared in step b, take 5 μL of the dispensing solution on the glassy carbon electrode, and dry overnight;
[0053] d.MCF-IL-Fe(CN) 6 3- / Preparation of PVA modified electrode
[0054] Put the glassy carb...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com