Wood preservative and preparation method thereof
A technology of wood preservative and polyethylene glycol, which is applied in wood treatment, impregnation of wood, wood impregnation, etc., can solve the problems of insects, easy decay of wood, etc., and achieve high safety, simple preparation process, and high-efficiency wood preservative effect Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0024] Another aspect of the present invention provides a method for preparing the above-mentioned wood preservative, the preparation method comprising: uniformly mixing nano-copper oxide, acetic acid, sodium borate, potassium sorbate, tebuconazole, polyethylene glycol and water to obtain the obtained wood preservatives.
[0025] As a preferred solution, all raw materials for preparing the preservative of the present invention can be obtained commercially.
[0026] According to the present invention, preferably, the preparation method includes: uniformly mixing the polyethylene glycol and water to obtain a mixed solution; adding the nano copper oxide, acetic acid, sodium borate, potassium sorbate and tebuconazole into the In the mixed liquid, mix evenly to obtain the wood preservative.
[0027] According to the present invention, preferably, the mixing speed is 100-200r / min, and the mixing time is 20-30min.
[0028] In the present invention, the prepared wood preservative is...
Embodiment 1
[0032] The present embodiment provides a wood preservative, in parts by mass, the wood preservative comprises: 15 parts of nano-copper oxide, 20 parts of acetic acid, 10 parts of sodium borate, 8 parts of potassium sorbate, 3 parts of tebuconazole, poly 10 parts of ethylene glycol and 10 parts of water.
[0033] The specific preparation method is: (1) uniformly mix the polyethylene glycol and water to obtain a mixed solution; wherein, the mixing speed is 150r / min, and the mixing time is 25min; (2) the nano-copper oxide, acetic acid, boric acid Sodium, potassium sorbate and tebuconazole were added into the mixed solution, and mixed uniformly to obtain the wood preservative; wherein, the mixing speed was 150 r / min, and the mixing time was 25 minutes.
Embodiment 2
[0035] The present embodiment provides a wood preservative, in parts by mass, the wood preservative comprises: 18 parts of nano-copper oxide, 23 parts of acetic acid, 12 parts of sodium borate, 10 parts of potassium sorbate, 3 parts of tebuconazole, poly 12 parts of ethylene glycol and 12 parts of water.
[0036] The specific preparation method is: (1) uniformly mix the polyethylene glycol and water to obtain a mixed solution; wherein, the mixing speed is 150r / min, and the mixing time is 25min; (2) the nano-copper oxide, acetic acid, boric acid Sodium, potassium sorbate and tebuconazole were added into the mixed solution, and mixed uniformly to obtain the wood preservative; wherein, the mixing speed was 150 r / min, and the mixing time was 25 minutes.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com