Ice-snow melting
A technology of ice and snow and calcium nitrate, applied in the field of compound salt, can solve the problems of slow snow removal, corrosion of metal and cement concrete, harmful plants and green space growth, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0053] Under the natural conditions of the highest temperature of -26°C, the lowest temperature of -33°C, and snowfall of 1.6mm; the external environment is: the downtown area, the greening is good, the road is covered with ice and snow, and the motor vehicles are driving intensively. The technical formula is: The weight content of each component is: (1=100kg / consumption)
[0054] Calcium chloride: 80 Magnesium chloride: 20
[0055] Sodium peroxide: 1.8 Sodium molybdate: 6
[0056] Sodium tripolyphosphate: 6 Sodium metasilicate: 3
[0057] The above-mentioned materials are put into the pulverizer in batches according to the weight of the components, and they are crushed and screened to make them reach the quality standard of 0.1mm ~ 8mm solid particles; Stir to mix all the materials evenly; finally, put the products that meet the quality standards into the spreading vehicle, and carry out the spreading operation on the implementation site, or pack the products that meet the ...
Embodiment 2
[0059] Under the natural conditions of the highest temperature of -16°C, the lowest temperature of -23°C, and snowfall of 1.3mm; the external environment is: the downtown area, the greening is good, the road is covered with ice and snow, and the motor vehicles are driving intensively. The technical formula is: The weight content of each component is: (1=100kg / consumption)
[0060] Water: 100 Calcium Nitrate: 70
[0061] Magnesium chloride: 30 Sodium molybdate: 6
[0062] Sodium tripolyphosphate: 6 Sodium hypochlorite: 1.8
[0063] Water quality stabilizer - PTX-CS: 0.001
[0064] First put the water in the reaction kettle, then place the above-mentioned materials in parts by weight, put them in the reaction kettle in batches, stir for ≥30 minutes, and then add the water quality stabilizer——PTX-CS to the solution In the process, stir for ≥10 minutes, let stand for ≥30 minutes, filter out the residue with a 120-mesh copper sieve, make liquid ice and snow melt, spray on the im...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com