Method for preparing roofing waterproof paint
A technology for waterproof coatings and base materials, applied in the direction of antifouling/underwater coatings, paints containing biocide, etc., can solve the problems of difficult construction, poor waterproof performance, poor high and low temperature elongation, etc., to facilitate transportation and construction, Good elongation and fast curing
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2008-01-30
- Estimated Expiration
- Not applicable · inactive patent
Abstract
Description
technical field
[0001] The invention relates to a preparation method of roof waterproof paint. Background technique
[0002] The existing asphalt, modified asphalt, and waterproof coatings made of waste rubber have poor high and low temperature elongation, poor waterproof performance, and difficult construction. Contents of the invention
[0003] The object of the present invention is to overcome above-mentioned defective, a kind of roof waterproof coating preparation method is provided.
[0004] The technical solution of the present invention is: a method for preparing roof waterproof coating, which is characterized in that: first inject 20-40% by weight vinyl acetate monomer into the reaction kettle, and gradually add 60-80% by weight to the stirring Finally, increase the stirring speed until the proportioned tar is added, and use sodium hydroxide to adjust the PH value to be alkaline. Ethylene release, curing in the sun.
[0005] The invention has the following advan...
Examples
Embodiment
[0006] Embodiment: a kind of preparation method of roofing waterproof paint, injecting weight percentage in reaction kettle is 20-40% vinyl acetate monomer first, and it is gradually added into the tar that weight percentage is 60-80% in its stirring, finally increases stirring speed to After adding the proportioned tar, use sodium hydroxide to adjust the PH value to be alkaline. This is used as the base material. Finally, dispersant, toughener, anti-aging agent, and water repellent are added in sequence, released with water, and cured in the sun.