A technology of water-based ink and manufacturing process, applied in the direction of ink, application, household appliances, etc., can solve the problems of peeling off wear-resistant paper and decorative paper, melamine can not produce cross-linking reaction, and melamine glue cannot penetrate and infiltrate.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] (1) Dissolve 10 grams of gelatin in 100 grams of deionized water, add 2 grams of NaHCo 3 or Na 2 co 3 , heated to above 60°C under full stirring.
[0019] (2) Take 2.5 grams of methyl methacrylate and emulsify with a small amount of emulsifier.
[0020] (3) emulsified methyl methacrylate and 1 gram (NH 4 ) 2 S 2 o 8 Simultaneously add slowly, after more than 2 hours, the dropwise addition is completed, heat up to above 80°C and keep warm for 2 hours, then cool to below 30°C and filter out.
[0021] (4) Add a small amount of thickener, leveling agent, defoamer, and alcohol solvent to form a vehicle for water-based ink.
[0022] (5) Water, pigments, dispersing aids, alcohol solvents, and a small amount of linking material are ground to prepare color paste. Pigments include red, yellow, blue, black, and titanium dioxide.
[0023] (6) Mix 80 grams of connecting material and 20 grams of color paste evenly, and the grinding fineness reaches 2-5 μm, and discharge to ob...
Embodiment 2
[0025] (1) Dissolve 10 grams of gelatin in 100 grams of deionized water, add 5 grams of NaHCo 3 , heated to above 70°C under full stirring.
[0026] (2) Take 2 grams of hexapropionamide and dissolve it with 10 grams of deionized water.
[0027] (3) dissolved caprolactam solution and 1 gram of K 2 S 2 o 8 At the same time, it is slowly added dropwise to the solution in step (1), and the dropwise addition is completed after 2 hours, and then cooled and discharged after being kept at 80°C for 2 hours.
[0028] (4) Add a small amount of thickener, leveling agent, defoamer, and alcohol solvent to form a vehicle for water-based ink.
[0029] (5) Water, pigments, dispersing aids, alcohol solvents, and a small amount of linking material obtained in step (4) are prepared by grinding to prepare color paste. Pigments include red, yellow, blue, black, and titanium dioxide.
[0030] (6) 50 grams of the connecting material obtained in step (4) and 50 grams of the color paste in step (5...
Embodiment 3
[0032] (1) Dissolve 10 grams of gelatin in 100 grams of deionized water, add 0.5 grams of Na 2 co 3 , heated to above 60°C under full stirring.
[0033] (2) 3 grams of styrene, 1.5 parts of hexapropionamide, mixed evenly, and emulsified with a small amount of emulsifier.
[0034] (3) the emulsion obtained in the above step (2) and 1 gram of K 2 S 2 o 8 At the same time, slowly add dropwise, after the dropwise addition is completed over 2 hours, add 1 g of tert-butyl hydroperoxide, raise the temperature to above 80°C and keep it warm for 2 hours, then cool to below 40°C and filter out.
[0035] (4) Add a small amount of thickener, leveling agent, defoamer, and alcohol solvent to form a vehicle for water-based ink.
[0036] (5) Water, pigments, dispersing aids, alcohol solvents, and a small amount of linking material obtained in step (4) are prepared by grinding to prepare color paste. Pigments include red, yellow, blue, black, and titanium dioxide.
[0037] (6) 60 grams o...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com