[0006] Although the above prior art has realized the coloring of wood, the operation steps are cumbersome, and the coloring may be too fake or not real enough. At the same time, after using simple dyes to color the wood, the wood will carry the dye to bring pungent smell, not environmentally friendly

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0025] The present embodiment provides a kind of wood coloring method, and this wood coloring method comprises:

[0026] (1) Cooking wood: cooking wood in a dye solution;

[0027] (2) Prepare wrapped peat: modify the peat in a constant temperature drying oven at 140°C, then soak the modified peat in a dye solution to obtain the wrapped peat;

[0028] (3) Baking and coloring: the wood is wrapped with peat, fixed with aluminum foil, dried, and the peat on the surface of the wood is removed to obtain the colored wood.

[0029] The initial density of wood is 0.5g / cm 3 .

[0030] In step (1), the cooking time is 20 minutes, and the wood is completely immersed in the dye solution during cooking.

[0031] In step (3), the thickness of the peat wrap is 8mm.

[0032] In the peat, the weight ratio of the peat with a particle size of 0.25-1 mm to the peat with a particle size of 1-2 mm is 3:1.

[0033] The baking temperature is 150° C., and the baking time is 200 minutes.

[0034] ...

Embodiment 2

[0036] The present embodiment provides a kind of wood coloring method, and this wood coloring method comprises:

[0037] (1) Cooking wood: cooking wood in a dye solution;

[0038] (2) Prepare wrapped peat: modify the peat in a constant temperature drying oven at 130°C, then soak the modified peat in a dye solution to obtain the wrapped peat;

[0039] (3) Baking and coloring: the wood is wrapped with wrapped peat, and the wrapped peat is fixed with aluminum foil, dried, and the colored wood is obtained after removing the peat on the wood surface.

[0040] The initial density of wood is 0.4g / cm 3 .

[0041] In step (1), the cooking time is 20 minutes, and the wood is completely immersed in the dye solution during cooking.

[0042] In step (3), the thickness of the peat wrapping is 5mm.

[0043] In the peat, the weight ratio of the peat with a particle size of 0.25-1mm to the peat with a particle size of 1-2mm is 2:1.

[0044] The baking temperature is 130° C., and the bakin...

Embodiment 3

[0047] The present embodiment provides a kind of wood coloring method, and this wood coloring method comprises:

[0048] (1) Cooking wood: cooking wood in a dye solution;

[0049] (2) Prepare wrapped peat: modify the peat in a constant temperature drying oven at 160°C, then soak the modified peat in a dye solution to obtain the wrapped peat;

[0050] (3) Baking and coloring: the wood is wrapped with peat, dried, and the peat on the surface of the wood is removed to obtain the colored wood.

[0051] The initial density of wood is 0.55g / cm 3 .

[0052] In step (1), the cooking time is 10 minutes, and the wood is completely immersed in the dye solution during cooking.

[0053] In step (3), the thickness of the peat wrap is 8mm.

[0054] In the peat, the weight ratio of the peat with a particle size of 0.25-1 mm to the peat with a particle size of 1-2 mm is 5:1.

[0055] In step (3), the coloring method further includes fixing the wrapped peat with aluminum foil.

[0056] Th...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses a wood staining method. The wood staining method comprises the following steps of (1) boiling of wood: boiling the wood in a dye liquid; (2) preparing of coating peat: modifying the peat in a constant-temperature drying box at the temperature of 130 to 160 DEG C, and soaking the modified peat into the dye liquid, so as to obtain the coating peat; (3) baking and staining: coating the wood by the coating peat, drying, and clearing the peat at the surface of the wood, so as to obtain the stained wood. The wood staining method has the advantages that the obtained wood is coated by the coating peat and then baked, the dye liquid gradually permeates into the wood, and the staining of the obtained stained wood is more uniform; after coating by the peat, the harmful mattersand irritation odor of the dye liquid are adsorbed by the peat, so that the obtained wood is environment-friendly and harmless; the operation procedures are simple, and the cost is greatly reduced.

Description

technical field [0001] The invention belongs to the technical field, and more specifically relates to a wood coloring method. Background technique [0002] Wood coloring is the method and processing process of using dyes, pigments and chemicals to obtain the required color of wood on the basis of maintaining the original properties of wood. [0003] Chinese patent application No. 201610344609.X discloses a wood penetrating coloring method. The dye solution is injected into an iron container, and then the uncolored wood is soaked in the dye solution; it is heated at a rate of 5°C / h to The temperature is 85-95°C, and it is kept at this temperature for 3-5 hours; after the heat preservation is completed, the temperature is naturally lowered to 40-60°C, and it is kept at this temperature for 72-144 hours; the wood is taken out to obtain an antique style. Distressed, stained wood. The method is suitable for coloring wood such as maple and oak; the color of the wood after colori...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): B27K5/02B27K5/04B27K5/00B27K3/12
CPCB27K3/12B27K5/001B27K5/02B27K5/04
Inventor 潘杰
Owner 芜湖瑞祥木业包装有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products