Embodiment 1
[0035] Example 1 : Preparation of Vegetable Salt Containing Sea Salt and Rhodiola Rosea Extract
[0036] step 1 , brine to remove heavy metals
[0037] (1) Precipitation filtration
[0038] Filtration: Take coastal brine, the content of tungsten ions is 26mg / L, the content of lead ions is 20mg / L, and the content of nickel ions is 22mg / L. Put the brine into the sedimentation tank and settle for 7 hours.
[0039] Mechanical filtration: the brine from which heavy metal ions have been removed is mechanically filtered to remove large solid impurities and mechanical impurities; the turbidity of the brine after filtration is 2NTU.
[0040] Nanofiltration: The mechanically filtered brine is subjected to nanofiltration treatment. The nanofiltration temperature should be controlled at 22°C and the pressure should be controlled at 0.6MPa.
[0041] A reducing agent is added to the nanofiltration process, and the reducing agent used is sodium sulfite, and the amount of the redu...
Embodiment 2
[0070] Example 2 : Preparation of Vegetable Salt Containing Sea Salt and Rhodiola Rosea Extract
[0071] step 1 , brine to remove heavy metals
[0072] (1) Precipitation filtration
[0073] Filtration: Take coastal brine, the content of tungsten ions is 26mg / L, the content of lead ions is 22mg / L, and the content of nickel ions is 20mg / L. Put the brine into the sedimentation tank and settle for 8 hours.
[0074] Mechanical filtration: The brine that removes heavy metal ions is mechanically filtered to remove large solid impurities and mechanical impurities; the turbidity of the brine after filtration is 3NTU.
[0075] Nanofiltration: The mechanically filtered brine is subjected to nanofiltration treatment, the nanofiltration temperature should be controlled at 23°C, and the pressure should be controlled at 0.6MPa.
[0076] A reducing agent is added to the nanofiltration process, and the reducing agent used is sodium sulfite, and the amount of the reducing agent adde...
Embodiment 3
[0104] Example 3 : Preparation of Vegetable Salt Containing Sea Salt and Rhodiola Rosea Extract
[0105] step 1 , brine to remove heavy metals
[0106] (1) Precipitation filtration
[0107] Filtration: Take coastal brine, the content of tungsten ions is 30mg / L, the content of lead ions is 20mg / L, and the content of nickel ions is 22mg / L. Put the brine into the sedimentation tank and settle for 9 hours.
[0108] Mechanical filtration: the brine from which heavy metal ions have been removed is mechanically filtered to remove large solid impurities and mechanical impurities; the turbidity of the brine after filtration is 2NTU.
[0109] Nanofiltration: The mechanically filtered brine is subjected to nanofiltration treatment, the nanofiltration temperature should be controlled at 21°C, and the pressure should be controlled at 0.8MPa.
[0110] A reducing agent is added to the nanofiltration process, and the reducing agent used is sodium sulfite, and the amount of the red...
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Particle size | aaaaa | aaaaa |
Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com