Composite restoration agent for water body as well as preparation method and application thereof
A composite restoration and water body technology, applied in separation methods, chemical instruments and methods, liquid separation, etc., can solve the problems of inability to release oxygen and effectively decompose pollutants in a long-term and efficient manner, so as to improve solubility, reduce surface tension, and increase dissolved oxygen The effect of content
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0044] Embodiment 1: A kind of water body composite restoration agent and preparation method thereof
[0045] A water body composite restoration agent is prepared from the following raw materials in parts by weight:
[0046] 40 parts of polyglycerin fatty acid ester;
[0047] 40 parts of iron powder;
[0048] 15 parts of activated carbon powder;
[0049] 35 parts of sodium bentonite;
[0050] Portland cement 20 parts;
[0051] The preparation process of the above-mentioned water body composite restoration agent: mix various raw materials such as polyglycerol fatty acid ester, iron powder, activated carbon powder, sodium-based bentonite, Portland cement, etc. in proportion, add an appropriate amount of water, and fully stir and mix; then mix the mixture Inject into a honeycomb mold, extrude to form a cube, then place it at room temperature, and keep it away from light for 7 days to obtain the finished repair agent.
Embodiment 2
[0052] Embodiment 2: A kind of water body composite restoration agent and preparation method thereof
[0053] A water body composite restoration agent is prepared from the following raw materials in parts by weight:
[0054] 35 parts of polyglycerin fatty acid ester;
[0055] 30 parts of iron powder;
[0056] 10 parts of activated carbon powder;
[0057] 25 parts of sodium bentonite;
[0058] Portland cement 15 parts;
[0059] The preparation process of the above-mentioned water body composite restoration agent: mix various raw materials such as polyglycerol fatty acid ester, iron powder, activated carbon powder, sodium-based bentonite, Portland cement, etc. in proportion, add an appropriate amount of water, and fully stir and mix; then mix the mixture Inject into a honeycomb mold, extrude to form a cube, then place it at room temperature, and keep it away from light for 7 days to obtain the finished repair agent.
Embodiment 3
[0060] Embodiment 3: the restoration agent prepared by the present invention is used for the test of the restoration of polluted water body
[0061]Trials were carried out in three 1 m x 1 m test tanks. In the same polluted lake, 30L of polluted lake water was poured into the experimental pool respectively, and the initial COD content and dissolved oxygen content of the lake water were detected, see Table 1. 30 g of the restorative agent prepared in Example 1 and Example 2 were respectively put into two of the test pools, and the other test pool was used as a control without adding the preparation.
[0062] During the test period, the air temperature was 25-30°C.
[0063] After 1 day (24h) and 3 days (72h), the COD content and dissolved oxygen content of the water body were detected respectively, and the results are shown in Table 2.
[0064] Table 1 Water quality indicators of polluted lake water
[0065] index COD (mg / L) Dissolved oxygen (mg / L) content b...