A technology of delayed coking and reaction tower, applied in the field of defoamer and high temperature resistant defoamer, can solve the problems of the influence of hydrotreating device and high silicon content in the product, and achieve the effect of inhibiting and foaming and eliminating foaming.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] Take 50 grams of modified polysiloxane compound A, 10 grams of phenyl silicone oil, and 40 grams of heavy aromatic solvent oil into a 250mL round bottom flask, heat at 60°C, and stir with magnetic force for 1 hour to obtain the product.
Embodiment 2
[0032] Take 20 grams of modified polysiloxane compound A, 20 grams of phenyl silicone oil, and 60 grams of heavy aromatic solvent oil into a 250mL round bottom flask, heat at 60°C, and stir with magnetic force for 1 hour to obtain the product.
Embodiment 3
[0034] Take 30 grams of modified polysiloxane compound A, 30 grams of phenyl silicone oil, and 40 grams of heavy aromatic solvent oil into a 250mL round bottom flask, heat at 60°C, and stir with magnetic force for 1 hour to obtain the product.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com