A kind of medical composite biomaterial application and preparation method
A technology of composite biological materials and biological materials, applied in the field of composite biological material application and composite biological materials, can solve the problems of unfavorable wound repair and high production cost, achieve good safety and biocompatibility, fast wound healing and repair , the effect of promoting growth
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] see figure 1 , a medical composite biomaterial application, which is composed of a base layer 1, a wound protection layer 2 and two peeling layers 3, the wound protection layer 2 is closely attached to the center of one side of the base layer 1, and the two peeling layers 3 One end is partially overlapped and covered on the wound-protecting layer 2 to protect the wound-protecting layer. The other ends of the two peeling layers 3 are bonded to the two ends of the base layer 1 for easy peeling during use. The base layer 1 and the wound-protecting layer 2. The corrugated non-woven medical air-permeable adhesive tape with a glue-carrying layer on the surface of the attached side, the wound protection layer 2 is a composite biomaterial, the composite material is made of silk fibroin porous biomaterial and chitosan, and the peeling layer 3 is Release paper, such as glassine paper.
Embodiment 2
[0027] Example 2 Preparation method of wound protection layer
[0028] (1) Raw silk degumming: configure 1% soapy water washing solution, which contains NaHCO with a mass concentration of 0.5% 3 , Soak raw silk in it, the weight ratio of silk to solution is 1:25, the soaking temperature is 70°C, the soaking time is 40 minutes, washed with deionized water, the water temperature is 70°C, soaked at constant temperature for 40 minutes, loosen the silk, and air-dry at room temperature, to spare;
[0029] (2) Preparation of silk fibroin porous biological material: The material obtained in step (1) is roughly opened; the speed is 0.20Hz feeding and transmission mode mixed with cotton; the speed is 0.20Hz fine opening; through the vacuum with metering pump Transfer box transfer, the conditions for controlling the vacuum transfer box are: the main cylinder speed is 20Hz, the doffer speed is 20Hz, and the messy speed is 14Hz; double-layer carding, the carding condition is that the cott...
Embodiment 3
[0034] Example 3 Preparation method of wound protection layer
[0035] 1) Raw silk degumming: configure 1% soapy water washing solution, which contains NaHCO with a mass concentration of 0.5% 3 , Soak raw silk in it, the weight ratio of silk to solution is 1:25, the soaking temperature is 90°C, the soaking time is 60 minutes, washed with deionized water, the water temperature is 90°C, soaked at constant temperature for 60 minutes, loosen the silk, and air-dry at room temperature, to spare;
[0036] 2) Preparation of silk fibroin porous biological material: The material obtained in step 1) is roughly opened; the speed is 0.40Hz feeding and transmission mode mixed with cotton; the speed is 0.40Hz fine opening; through the vacuum transfer box with a metering pump Transfer, the conditions for controlling the vacuum transfer box are: the main cylinder speed is 30Hz, the doffer speed is 30Hz, and the messy speed is 19 Hz; double-layer carding, the carding condition is that the cott...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com