[0023] The present invention provides a kind of preparation method of rare earth yttrium air cleaner, comprises following component:
[0024]
[0025] Prepared by the following steps:
[0026] Step 1: Prepare the chlorine dioxide solution, put it into a PE plastic bottle, put the activator, slow-release agent, and gel into a glass container and stir evenly, wait for 5-8 minutes to stir, and when the color of the reagent is uniform, put Pour the well-stirred reagent into the chlorine dioxide solution in the PE plastic bottle. The reagent diffuses automatically in the solution and can be mixed without stirring. Keep in a cool and ventilated place indoors.
[0027] Step 2: After standing for 1-2 days, the gel-like reagent becomes a soft solid, take out the solid, put it into a high-pressure micro-powder mill, and grind it into a powder with a particle size of 5-20 nanometers, and collect the powder in a plastic bag .
[0028] Step 4: Add activated carbon powder and photocat...
Embodiment 2
[0031] The present invention provides a kind of preparation method of rare earth yttrium air cleaner, comprises following component:
[0032]
[0033] Prepared by the following steps:
[0034] Step 1: Prepare the chlorine dioxide solution, put it into a PE plastic bottle, put the activator, slow-release agent, and gel into a glass container and stir evenly, wait for 5-8 minutes to stir, and when the color of the reagent is uniform, put Pour the well-stirred reagent into the chlorine dioxide solution in the PE plastic bottle. The reagent diffuses automatically in the solution and can be mixed without stirring. Keep in a cool and ventilated place indoors.
[0035] Step 2: After standing for 1-2 days, the gel-like reagent becomes a soft solid, take out the solid, put it into a high-pressure micro-powder mill, and grind it into a powder with a particle size of 5-20 nanometers, and collect the powder in a plastic bag .
[0036] Step 4: Add activated carbon powder and photocat...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com