A kind of sulfonated residual oil modified bentonite foam stabilizer and preparation method thereof
A technology of sulfonated residue and bentonite, which is applied in the field of sulfonated residue modified bentonite foam stabilizer and its preparation, can solve problems such as prominent plane and vertical conflicts, poor reservoir development effect, etc., and achieve suspension improvement, Good balance between hydrophilic and lipophilic, good compatibility
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0041] This embodiment has prepared a kind of sulfonated residual oil modified bentonite foam stabilizer, and the preparation steps are:
[0042] (1) At room temperature, put residual oil and bentonite (sodium-based bentonite) with a mass ratio of 1:1 in a beaker, then add solvent dichloromethane (the mass ratio of dichloromethane and residual oil is 1:1) to carry out Stir for 1h to obtain a mixture;
[0043] (2) After the solvent in the mixture is volatilized, the bentonite coated with residual oil is obtained;
[0044] (3) A three-necked flask equipped with a stirrer, a thermometer and a dropping funnel is fixed in a constant temperature water bath, and the bentonite coated with residual oil is added to the three-necked flask;
[0045] (4) At 20°C, slowly add concentrated sulfuric acid (the mass ratio of residual oil to concentrated sulfuric acid is 1:1) from the dropping funnel, and control the dropping rate to 1 drop / s;
[0046] (5) Continue stirring reaction after dropw...
Embodiment 2
[0051] This embodiment has prepared a kind of sulfonated residual oil modified bentonite foam stabilizer, and the preparation steps are:
[0052](1) At room temperature, put residual oil and bentonite (sodium-based bentonite) with a mass ratio of 2:1 in a beaker, then add solvent chloroform (the mass ratio of chloroform and residual oil is 1.5:1) to carry out Stir for 1h to obtain a mixture;
[0053] (2) After the solvent in the mixture is volatilized, the bentonite coated with residual oil is obtained;
[0054] (3) A three-necked flask equipped with a stirrer, a thermometer and a dropping funnel is fixed in a constant temperature water bath, and the bentonite coated with residual oil is added to the three-necked flask;
[0055] (4) At 30°C, slowly add concentrated sulfuric acid (the mass ratio of residual oil to concentrated sulfuric acid is 3:1) from the dropping funnel, and control the dropping rate to 1 drop / s;
[0056] (5) Continue stirring reaction after dropwise addit...
Embodiment 3
[0061] This embodiment has prepared a kind of sulfonated residual oil modified bentonite foam stabilizer, and the preparation steps are:
[0062] (1) At room temperature, put residual oil and bentonite (sodium bentonite) with a mass ratio of 3:1 in a beaker, then add solvent ethanol (the mass ratio of ethanol to residual oil is 1:1) and stir for 1.5h, get the mixture;
[0063] (2) After the solvent in the mixture is volatilized, the bentonite coated with residual oil is obtained;
[0064] (3) A three-necked flask equipped with a stirrer, a thermometer and a dropping funnel is fixed in a constant temperature water bath, and the bentonite coated with residual oil is added to the three-necked flask;
[0065] (4) At 40°C, slowly add concentrated sulfuric acid (the mass ratio of residual oil to concentrated sulfuric acid is 3:1) from the dropping funnel, and control the dropping rate to 1 drop / s;
[0066] (5) continue stirring reaction after dropwise addition, stop stirring after...