A foam board and hollow technology, which is applied in the field of formula system of wide hollow foam board, can solve the problems of poor antistatic performance and poor flame retardancy, so as to increase flame retardancy and solve poor flame retardancy , Solve the effect of poor antistatic performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A formulation system suitable for wide-width hollow foam boards, made of raw materials in the following weight ratio: 120 parts of PVC resin powder, 15 parts of nano-titanium dioxide, 15 parts of nano-calcium carbonate, 15 parts of nano-silicon carbide, and modified asbestos 15 parts of fiber, 12 parts of nano-calcium silicate hydrate, 10 parts of foaming agent, 1.2 parts of flame retardant, and 0.8 part of antistatic agent.
[0022] Among them, the preparation method of the modified asbestos fiber is as follows: the asbestos fiber is ultrasonically crushed to treat the asbestos fiber for 30 minutes; the pulverized asbestos fiber is dried in an oven at a temperature of 1200-1500 ° C for 4 hours; and then the temperature of the oven is lowered to 150 ℃, keep warm for 24h, then cool the pulverized asbestos fibers to room temperature, put NH 4 Soak in Cl aqueous solution for 24 hours, then vacuum dry at low temperature until the moisture content is lower than 8%, to obtain...
Embodiment 2
[0027] A formulation system suitable for wide-width hollow foam boards, which is made of the following raw materials in the weight ratio: 100 parts of PVC resin powder, 10 parts of nano-titanium dioxide, 10 parts of nano-calcium carbonate, 10 parts of nano-silicon carbide, and modified asbestos 10 parts of fiber, 10 parts of nano calcium silicate hydrate, 12 parts of foaming agent, 0.5 part of flame retardant, 0.2 part of antistatic agent.
[0028] Among them, the preparation method of the modified asbestos fiber is as follows: the asbestos fiber is ultrasonically crushed to treat the asbestos fiber for 30 minutes; the pulverized asbestos fiber is dried in an oven at a temperature of 1200-1500 ° C for 4 hours; and then the temperature of the oven is lowered to 150 ℃, keep warm for 24h, then cool the pulverized asbestos fibers to room temperature, put NH 4 Soak in Cl aqueous solution for 24 hours, then vacuum dry at low temperature until the moisture content is lower than 8%, t...
Embodiment 3
[0033] A formula system suitable for wide-width hollow foam boards, made of raw materials in the following weight ratio: 110 parts of PVC resin powder, 12 parts of nano-titanium dioxide, 13 parts of nano-calcium carbonate, 13 parts of nano-silicon carbide, and modified asbestos 13 parts of fiber, 11 parts of nano-calcium silicate hydrate, 11 parts of foaming agent, 1 part of flame retardant, and 0.6 part of antistatic agent.
[0034] Among them, the preparation method of the modified asbestos fiber is as follows: the asbestos fiber is ultrasonically crushed to treat the asbestos fiber for 30 minutes; the pulverized asbestos fiber is dried in an oven at a temperature of 1200-1500 ° C for 4 hours; and then the temperature of the oven is lowered to 150 ℃, keep warm for 24h, then cool the pulverized asbestos fibers to room temperature, put NH 4 Soak in Cl aqueous solution for 24 hours, then vacuum dry at low temperature until the moisture content is lower than 8%, to obtain modifi...