Leather material having magnetic health care function and its application
A magnetic health care, magnetic material technology, applied in the application, leather impregnation, small raw hide/large raw hide/leather/fur treatment, etc., can solve the problem of less development and application, and achieve the promotion of human health, the balance of the magnetic field, and the improvement of blood The effect of microcirculation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1-3
[0049] According to the formula in Table 1, add the magnetic powder and anion powder to the high-speed stirrer and stir at low speed. Slowly add the coupling agent from the feeding port. Use high stirring to treat the powder for 15 minutes, and the high stirring speed is not less than 3000 rpm. The synthetic leather raw materials are added to the high stirring, mixed uniformly at low speed, and then the dispersant is added, mixed uniformly, and discharged. The raw materials are processed according to the normal synthetic leather production process to obtain a synthetic leather product containing magnetic particles.
[0050] Among them, strontium iron oxide, barium oxide iron, and neodymium iron boron were purchased from Beikuang Magnetic Materials Technology Co., Ltd. The performance of the magnetic powder is: the particle size is less than 5μm, the maximum coercive force iHc is greater than or equal to 240 (KA / m), the residual magnetic Br is greater than or equal to 140mT a...
Embodiment 4-6
[0061] The components and contents are as above, and the preparation method is the same as that in Examples 1-3.
[0062] Item
Embodiment 7-9
[0065] Respectively add the magnetic powder, anion powder, dispersant and other above-mentioned ingredients according to Table 5, add the high-speed stirrer to low-speed stirring, slowly add the coupling agent from the feeding port, use high stirring to treat the powder for 15 minutes, and the high stirring speed is not low Mix evenly at 3000 rpm, discharge the material, and then add it in the tanning process of sheepskin, pigskin, cowhide and other leathers, and perform the tanning process together to prepare a material with magnetic health care function. Other process conditions and steps adopt current There is a preparation process of leather materials.
[0066] The obtained dermal material containing magnetic particles is magnetized in a magnetizer to obtain a magnetic dermal material capable of emitting magnetic lines of force. The magnetic field performance test (magnetic flux and magnetic field intensity test) of the magnetic synthetic leather material is measured by ...
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com