Production process of wooden door

A production process and technology for wooden doors, applied in the direction of wood processing appliances, manufacturing tools, etc., can solve the problems of insufficient air tightness between paint and solid wood doors, door leaves are easily affected by weather, damp and moldy deformation, etc., and achieve excellent anti-deformation performance, Excellent waterproof and moisture-proof performance, not easy to deform and fall off

Inactive Publication Date: 2018-12-18
中山市宝润木业有限公司
View PDF8 Cites 7 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Mainly rely on the properties of the paint to improve the surface performance of the solid wood door. Because the combination of the paint and the solid wood door is not airtight enough, the door leaf is easily affected by the weather, resulting in dry cracking or damp mold deformation

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0020] A kind of production technology of wooden door, comprises the following steps:

[0021] S1, wood drying and cutting

[0022] The wood is sprayed and steamed and then baked so that the moisture content of the wood is 8-12%;

[0023] S2, door panel treatment

[0024] The door panel is carved and planed, and then a polyvinyl chloride film is laid on the surface of the door panel, and then put into a blister machine for blister molding. The temperature in the blister machine is 220-226°C, and the blister time is 80-90s. The surface of the door panel is pasted with a polyvinyl chloride transparent film layer. The polyvinyl chloride film is composed of the following components by mass percentage: 95.78% polyvinyl chloride resin, 4% dioctyl adipate, 0.2% isooctyl dimethyltin dithioacetate, 0.02% coloring agent .

[0025] S3, Histoembryo suppression

[0026] Combine the wood into the door core, apply glue and attach the door panel, and then use a cold press machine or a co...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention provides a production process of a wooden door. The production process comprises the following steps that S1, wood is dried and blanked, baking treatment is carried out after the wood issubjected to spray steaming, and the moisture content of the wood ranges from 8% to 12%; S2, door plate treatment is carried out, wherein a door plate is carved and dressed, then a polyvinyl chloridefilm is laid on the surface of the door plate, and then the door plate is placed in a plastic vacuum forming machine to be subjected to plastic vacuum forming, so that a polyvinyl chloride transparent film is pasted on the surface of the door plate; S3, assembling and pressing are carried out, wherein the wood is combined to form a door core, after the door plate is coated with glue, cold pressing and pressure maintaining are carried out till the glue layer is cured, and a preliminarily formed door leaf is obtained; and S4, paint spraying and grinding are carried out, wherein paint is sprayedto the surface of the door leaf, and the unsmooth paint face is ground after airing is carried out. According to the production process of the wooden door, the manufactured door leaf is good in sealing performance, excellent waterproof and dampproof performance is achieved, and the situation of drying and cracking can be avoided.

Description

technical field [0001] The invention relates to a production process of a wooden door. Background technique [0002] Solid wood doors refer to the materials used to make wooden doors are natural logs or solid wood laminates from forests. Most of the existing solid wood doors are processed through processes such as drying, blanking, planing, milling, assembling, polishing, and painting. Mainly rely on the properties of the paint to improve the surface performance of the solid wood door. Due to the insufficient airtightness of the combination of the paint and the solid wood door, the door leaf is easily affected by the weather, resulting in dry cracking or damp moldy deformation. Contents of the invention [0003] In order to overcome the deficiencies of the prior art, the present invention proposes a production process for wooden doors. The resulting door leaf has good airtightness, excellent waterproof and moisture-proof performance, and can prevent drying and cracking. ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): B27M3/18
CPCB27M3/18
Inventor 司徒立权
Owner 中山市宝润木业有限公司
Who we serve
  • R&D Engineer