Water-based environment-friendly inner wall heat physiotherapeutic paint and preparation method thereof
An environmental protection, interior wall technology, applied in the field of coatings, can solve problems such as lack of availability, and achieve the effects of improving blood circulation, improving air quality, and inhibiting oxidation or aging
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0028] Embodiment 1 Preparation of water-based environmental protection interior wall heating physiotherapy paint
[0029] (1) Raw material ratio
[0030] The ratio of raw materials for preparing the water-based environmental protection interior wall heating physiotherapy coating is as follows: by weight percentage, 25% of deodorant emulsion, 15% of titanium dioxide, 6% of filler, 6% of far-infrared ceramic powder, 9% of tourmaline powder, and 0.4% of cellulose , Wetting agent 0.2%, dispersant 0.5%, neutralizer 0.1%, defoamer 0.2%, antiseptic bactericide 0.4%, thickener 0.7%, water 36.5%.
[0031] Among them, the titanium dioxide is anatase titanium dioxide, the whiteness is more than 94%, and Henan Billions titanium dioxide BLA-200 is selected; the filler is kaolin; 250HBR; wetting agent is selected from BASF WE 3111; the dispersant is sodium polycarboxylate, LOPON 800 is selected; the neutralizing agent is 2-amino-2-methyl-1-propanol, AMP-95 is selected; the defoamer is m...
Embodiment 2
[0036] Embodiment 2 Preparation of water-based environmental protection interior wall heating physiotherapy paint
[0037] The ratio of raw materials for preparing the water-based environmental protection interior wall heating physiotherapy coating is as follows: by weight percentage, 29% of deodorant emulsion, 13% of titanium dioxide, 7% of filler, 7% of far-infrared ceramic powder, 8% of tourmaline powder, and 5% of cellulose , Wetting agent 0.2%, dispersant 0.5%, neutralizer 0.2%, defoamer 0.3%, antiseptic bactericide 0.5%, thickener 0.8%, water 28.5%.
[0038] Among them, the titanium dioxide is anatase titanium dioxide, the whiteness is greater than 94%, and Henan Billions titanium dioxide BLA-200 is selected; the filler is heavy calcium; the cellulose is hydroxyethyl cellulose, and the American subtranslong hydroxyethyl Cellulose 250HBR; wetting agent selected from BASF WE 3111; dispersant is sodium polycarboxylate, LOPON 800 is selected; neutralizer is 2-amino-2-methy...
Embodiment 3
[0043] Embodiment 3 Preparation of water-based environmental protection interior wall heating physiotherapy paint
[0044] The ratio of raw materials for preparing the water-based environmental protection interior wall heating physiotherapy coating is as follows: by weight percentage, 31% of deodorant emulsion, 11% of titanium dioxide, 6% of filler, 8% of far-infrared ceramic powder, 7% of tourmaline powder, and 0.5% of cellulose , Wetting agent 0.3%, dispersant 0.6%, neutralizer 0.2%, defoamer 0.4%, antiseptic bactericide 0.6%, thickener 0.9%, water 33.5%.
[0045] Among them, the titanium dioxide is anatase titanium dioxide, the whiteness is greater than 94%, and Henan Billions titanium dioxide BLA-200 is selected; the filler is heavy calcium; the cellulose is hydroxyethyl cellulose, and the American subtranslong hydroxyethyl Cellulose 250HBR; wetting agent selected from BASF WE 3111; dispersant is polycarboxylate sodium salt, LOPON 800 is selected; neutralizer is 2-amino-...
PUM
Property | Measurement | Unit |
---|---|---|
whiteness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com