Evaluating methods of concrete surface coatings to extend the durability life of concrete structures
A concrete structure and concrete surface technology, applied in the direction of surface/boundary effect, weather resistance/light resistance/corrosion resistance, instruments, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment
[0027] Taking the 5-year exposure data in the splash zone of Qingdao Exposure Test Station as an example, the coating is calculated to prolong the service life of the concrete structure.
[0028] Assuming that the service life of the coating itself is 20 years, the coating will fail after 20 years and lose its protective effect; the thickness of the concrete protective layer is 50mm. Within the protection period of the coating, the average chloride ion concentration on the surface of the coated concrete is calculated by the following formula. The average surface concentration of chloride ions on the surface of the coated concrete for 20 years is 0.191 (%, relative to the mass percentage of the concrete).
[0029] (1)
[0030] = 0.191 (%, relative to the mass percentage of concrete)
[0031] Within the protection period of the coating, the average diffusion coefficient of the coated concrete is 0.11×10 -12 m 2 / s.
[0032] (2)
[0033] = 0.11 (×10 -12 m 2 / s)
...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com