Engine lubricating oil dispersing additive
A technology for engines and lubricating oils, applied in the direction of additives, lubricating compositions, petroleum industry, etc., which can solve the problems that the use and manufacture of additives cannot achieve the desired effect and the price is expensive, and achieve the maintenance of oil quality, simple preparation, and good low-temperature performance Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] An engine lubricating oil dispersant additive is composed of base oil; polyisobutylene bisbutyrimide; sulfurized alkyl powder calcium; diarylamine and hindered phenol mixture. The base oil is a mixture of 150BS, M14 and minus four lines. The weight ratio of the three components is 1:1:1. The mixture of two components of diarylamine and hindered phenol, the weight ratio of the two components is 1:1, the temperature is controlled between 40-50 DEG C during mixing, and the mixture is stirred for 120 minutes. The weight percent of each component is: base oil 26%; polyisobutylene bisbutyrimide 45%; sulfurized alkyl powder calcium 8%; polyisobutene amine 9%; diarylamine and hindered phenol mixture 12% The above-mentioned base oil; polyisobutylene bisbutyrimide; sulfurized alkyl powder calcium; Between 45-50°C, stir for 120 minutes. After filtering, the product of the present invention is produced.
[0014] This product is added to ordinary lubricating oil according to the...
Embodiment 2
[0020] An engine lubricating oil dispersant additive is composed of base oil; polyisobutylene bisbutyrimide; sulfurized alkyl powder calcium; diarylamine and hindered phenol mixture. The base oil is a mixture of 150BS and 5 centistokes. The weight ratio of the two components is 1:1. The mixture of two components of diarylamine and hindered phenol, the weight ratio of the two components is 1:1, the temperature is controlled between 40-50 DEG C during mixing, and the mixture is stirred for 120 minutes. The weight percent of each component is: base oil 19%; polyisobutylene bisbutyrimide 47%; sulfurized alkyl powder calcium 10%; polyisobutene amine 10%; mixture of diarylamine and hindered phenol 14% The above-mentioned base oil; polyisobutylene bisbutyrimide; sulfurized alkyl powder calcium; Between 45-50°C, stir for 300 minutes. After filtering, the product of the present invention is produced.
[0021] This product is added to ordinary lubricating oil according to the dosage...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap