Hair care composition with hair style fixing capacity
A hair care composition and the technology of ability, applied in the field of hair care composition with styling ability, can solve the problems of dry hair, deformed hair quality, no repair, etc., and achieve natural lubricating luster, natural styling, and good protection Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0024] Example 1: Preparation of the hair care composition of the present invention
[0025] Prepare the hair care composition according to the ingredients and proportions in Table 1.
[0026] Table I:
[0027] Element
[0028] First heat deionized water, vinylpyrrolidone / ethyl acetate copolymer (60 / 40), polyquaternium-4, glycerin and polysorbate-60 to 80-85°C, and also heat mineral oil to 80-85°C, then mix and emulsify the two for 3 minutes, keep warm for 10 minutes, cool to 45-50°C, add hydrolyzed pansy extract and preservative, stir evenly, and send for inspection.
Embodiment 2
[0029] Example 2: Preparation of the hair care composition of the present invention
[0030] Prepare the hair care composition according to the ingredients and proportions in Table 2.
[0031] Table II:
[0032] Element
[0033] Vinylpyrrolidone / vinyl acetate / vinyl propionate copolymer
[0034] First heat deionized water, vinylpyrrolidone / vinyl acetate / vinyl propionate copolymer, polyquaternium-28, glycerin and polysorbate-60 to 80-85°C, and at the same time, polysiloxane Heat to 80-85°C, then mix and emulsify and homogenize the two for 3 minutes, keep warm for 10 minutes, cool to 45-50°C, add hydrolyzed pansy extract and preservative, stir evenly, and send for inspection.
Embodiment 3
[0035] Example 3: Preparation of the hair care composition of the present invention
[0036] Prepare the hair care composition according to the ingredients and proportions in Table 3.
[0037] Table three:
[0038] Element
[0039] First heat deionized water, vinylpyrrolidone / ethyl acetate copolymer (70 / 30), polyquaternium-37, glycerin and polysorbate-60 to 80-85 ° C, and also hydrogenated polydecene Heat to 80-85°C, then mix and emulsify and homogenize the two for 3 minutes, keep warm for 10 minutes, cool to 45-50°C, add hydrolyzed pansy extract and preservative, stir evenly, and send for inspection.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology