A thin plate stamping and lubricating oil technology, which is applied in the field of stamping processing, can solve the problems of uneven oil quantity, discontinuity, and non-environmental protection, and achieve the effects of large adsorption force, improved deformation degree, and meeting environmental protection requirements
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] The raw materials and consumption of this embodiment configuration thin plate punching deep drawing lubricating oil are: 45 kilograms of palm oils, 35 kilograms of castor oils, 0.5 kilograms of antioxidants, 1 kilogram of antiwear agents, 1 kilogram of antirust agents, 5 kilograms of extreme pressure agents, Foam agent 3 kg.
[0016] The production steps are:
[0017] A. Weigh out each raw material respectively according to the above weight, and set aside;
[0018] B. Put the palm oil and castor oil into the container, stir while heating, when the temperature rises to 80°C, keep the temperature and stir for 20 minutes;
[0019] C. When continuing to heat up to 125°C, add antioxidant, antiwear agent, antirust agent, extreme pressure agent and defoamer, stir evenly, and obtain the required lubricating oil after cooling.
Embodiment 2
[0021] The raw materials and consumption of the preparation method of the thin plate stamping deep drawing lubricating oil configured in this embodiment are: 40 kg of palm oil, 25 kg of castor oil, 0.3 kg of antioxidant, 0.5 kg of antiwear agent, 0.5 kg of rust inhibitor, and 3 kg of extreme pressure agent kg, 2 kg of silicone defoamer.
[0022] The production steps are:
[0023] A. Weigh out each raw material respectively according to the above weight, and set aside;
[0024] B. Put palm oil and castor oil into the container, stir while heating, when the temperature rises to 80°C, keep the temperature and stir for 22 minutes;
[0025] C. When continuing to heat up to 128°C, add antioxidant, anti-wear agent, anti-rust agent, extreme pressure agent and defoamer, stir evenly, and obtain the required lubricating oil after cooling.
Embodiment 3
[0027] The raw materials and consumption of the preparation method of the thin plate stamping deep drawing lubricating oil configured in this embodiment are: 45 kg of palm oil, 30 kg of castor oil, 0.4 kg of antioxidant, 0.8 kg of antiwear agent, 0.8 kg of antirust agent, and 4 kg of extreme pressure agent kg, 2.5 kg of silicone defoamer.
[0028] The production steps are:
[0029] A. Weigh out each raw material respectively according to the above weight, and set aside;
[0030] B. Put palm oil and castor oil into the container, stir while heating, when the temperature rises to 80°C, keep stirring for 25 minutes at the temperature;
[0031] C. When continuing to heat up to 130°C, add antioxidant, anti-wear agent, anti-rust agent, extreme pressure agent and defoamer, stir evenly, and obtain the required lubricating oil after cooling.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More