Embodiment 1
[0032] First use the following steps to make water plant mud 1:
[0033] ①. Collect the river bottom silt and put it in the sun to expose it to the sun, control the water content of the silt to 30%, and then keep stirring to make mature mud;
[0034] 2. Spread the cooked mud and continue to expose to the sun. When the water content is 5%, rub the mud into small mud particles with a diameter of about 1 mm, and dry the mud particles in the shade;
[0035] ③. Mix 80 kg of coal and 30 kg of loess and crush them into small particles with a diameter of about 3 mm;
[0036] ④. Mix the pulverized coal particles and loess with 100 kg of shade-dried mud particles, and calcinate at 700°C for 34 hours;
[0037] ⑤. After cooling, sieve out coal ash to obtain 1 granule of water plant mud.
[0038] Then make the bottle cap 4 of the ecological ornamental bottle, install the battery tank 7 on the top of the ornamental bottle, bond the lighting lamp 5 on the lower surface of the viewing bottl...
Embodiment 2
[0042] First use the following steps to make water plant mud 1:
[0043] ①. Collect the river bottom silt and place it in the sun to expose it to the sun, control the water content of the silt to 40%, and then keep stirring to make mature mud;
[0044] 2. Spread the cooked mud and continue to expose to the sun. When the water content is 15%, rub the mud into small mud particles with a diameter of about 3mm, and dry the mud particles in the shade;
[0045] ③. Mix 100 kg of coal and 40 kg of loess and crush them into small particles with a diameter of about 3 mm;
[0046] ④. Mix the pulverized coal particles and loess with 100 kg of shade-dried mud particles, and calcinate at 800°C for 37 hours;
[0047] ⑤. After cooling, sieve out coal ash to obtain 1 granule of water plant mud.
[0048] Then make the bottle cap 4 of the ecological ornamental bottle, install the battery tank 7 on the top of the ornamental bottle, bond the lighting lamp 5 on the lower surface of the viewing bo...
Embodiment 3
[0052] First use the following steps to make water plant mud 1:
[0053] ①. Collect the river bottom silt and put it in the sun to expose it to the sun, control the water content of the silt to 40%, and then keep stirring to make mature mud;
[0054] 2. Spread the cooked mud and continue to expose to the sun. When the water content is 15%, rub the mud into small mud particles with a diameter of about 3mm, and dry the mud particles in the shade;
[0055] ③. Mix 100 kg of coal and 40 kg of loess and crush them into small particles with a diameter of about 3 mm;
[0056] ④. Mix the pulverized coal particles and loess with 100 kg of shade-dried mud particles, and calcinate at 800°C for 37 hours;
[0057] ⑤. After cooling, sieve out the coal ash to obtain water plant mud (1) granules.
[0058] Then make the bottle cap 4 of the ecological ornamental bottle, install the battery tank 7 on the top of the ornamental bottle, bond the lighting lamp 5 on the lower surface of the viewing bo...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com