Composite memory carrier and preparation method thereof as well as quantum water treatment process and quantum water treater based on carrier
A water processor, quantum water technology, applied in water/sewage treatment, adsorption water/sewage treatment, light water/sewage treatment, etc., can solve the problem of inability to apply quantum water treatment technology, and achieve wide application and simple structure , the effect of easy installation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0039] A preparation method of a composite memory carrier, comprising the steps of:
[0040] S1, weigh 40g of tourmaline, 1.5g of fatty alcohol polyoxyethylene ether sodium sulfate (AES), 5.8g of activated carbon, 35g of quartz and 17.7g of calcite;
[0041] S2, grinding and pulverizing the tourmaline, quartz and calcite in S1 into powder;
[0042] S3, add the powder in S2 into water, stir, add AES and activated carbon in S1 in sequence when the system is heated to 55°C, and react at constant temperature for 5 hours;
[0043] S4, suction filter the system after the reaction of S3, wash the filter residue, and dry;
[0044] S5, calcining the dried solid in S4 at a high temperature of 800° C. to form a composite memory carrier.
Embodiment 2
[0046] A preparation method of a composite memory carrier, comprising the steps of:
[0047] S1, weigh 55.6g of tourmaline, 1g of sodium dodecyl sulfate (SDS), 10g of activated carbon, 23g of quartz and 10.4g of calcite;
[0048] S2, grinding and pulverizing the tourmaline, quartz and calcite in S1 into powder;
[0049] S3, add the powder in S2 into water, stir, add sodium lauryl sulfate and activated carbon in S1 in sequence when the system is heated to 50°C, and react at constant temperature for 6 hours;
[0050] S4, suction filter the system after the reaction of S3, wash the filter residue, and dry;
[0051] S5, calcining the dried solid in S4 at a high temperature of 900° C. to form a composite memory carrier.
Embodiment 3
[0053] A preparation method of a composite memory carrier, comprising the steps of:
[0054] S1, weigh 45g of tourmaline, 2g of ethoxylated fatty acid methyl ester sulfonate (FMES), 7g of activated carbon, 26g of quartz and 20g of calcite;
[0055] S2, grinding and pulverizing the tourmaline, quartz and calcite in S1 into powder;
[0056] S3, add the powder in S2 into water, stir, add FMES and activated carbon in S1 in sequence when the system is heated to 55°C, and react at constant temperature for 6 hours;
[0057] S4, suction filter the system after the reaction of S3, wash the filter residue, and dry;
[0058] S5, calcining the dried solid in S4 at a high temperature of 950° C. to form a composite memory carrier.