Acid-corrosion-resistant X70MS pipeline steel hot rolled coil and manufacturing method thereof

A manufacturing method and pipeline steel technology, applied in the field of metal smelting, can solve the problems of hydrogen-induced cracking, increased alloy cost, stress corrosion cracking, etc., and achieve the effects of reducing segregation, high product competitiveness, and good economic benefits

A manufacturing method and pipeline steel technology, applied in the field of metal smelting, can solve the problems of hydrogen-induced cracking, increased alloy cost, stress corrosion cracking, etc., and achieve the effects of reducing segregation, high product competitiveness, and good economic benefits

CN109082601AInactive Publication Date: 2018-12-25BENGANG STEEL PLATES

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Acid-corrosion-resistant X70MS pipeline steel hot rolled coil and manufacturing method thereof
  • Acid-corrosion-resistant X70MS pipeline steel hot rolled coil and manufacturing method thereof
  • Acid-corrosion-resistant X70MS pipeline steel hot rolled coil and manufacturing method thereof

Examples

Experimental program
Comparison scheme
Effect test

Embodiment Construction

[0020] In order to make the object, technical solution and advantages of the present invention more clear, the present invention will be further described in detail below in conjunction with the examples. It should be understood that the specific embodiments described here are only used to explain the present invention, not to limit the present invention.

[0021] The invention provides an acid corrosion-resistant X70MS pipeline steel hot-rolled coil, which comprises the following components in terms of mass percentage: C: 0.03-0.10%; Mn: 1.10-1.40%; Si: 0.10-0.20%; Al: 0.010- 0.030%; Cr: 0.15-0.55%; Mo: 0.15-0.45%; Ti: 0.005-0.025%; Nb: 0.050-0.080%; V: 0.020-0.040%; Ni: 0.15-0.30%; P≤0.012%; S≤0.0020%; N≤0.0060%; O≤0.0018%; H≤0.0005%; the balance is Fe and unavoidable inclusions.

[0022] In order to obtain good comprehensive properties of acid corrosion-resistant X70MS pipeline steel, the molten steel must have good purity and low C content to reduce segregation and inclus...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
thicknessaaaaaaaaaa
Login to View More

Abstract

The invention provides an acid-corrosion-resistant X70MS pipeline steel hot rolled coil and a manufacturing method thereof. The acid-corrosion-resistant X70MS pipeline steel hot rolled coil comprisesthe following components including, by mass, 0.03% to 0.10% of C, 1.10% to 1.40% of Mn, 0.10% to 0.20% of Si, 0.010% to 0.030% of Al, 0.15% to 0.55% of Cr, 0.15% to 0.45% of Mo, 0.005% to 0.025% of Ti, 0.050% to 0.080% of Nb, 0.020% to 0.040% of V, 0.15% to 0.30% of Ni, not larger than 0.0002% of B, not larger than 0.012% of P, not larger than 0.0020% of S, not larger than 0.0060% of N, not largerthan 0.0018% of O, not larger than 0.0005% of H and the balance Fe and inevitable inclusions. Compositions and mechanical property of the acid-corrosion-resistant pipeline steel X70MS products meet the API 5L standard, the acid corrosion resistance performance meets international HIC resistant and SSCC resistant related standard requirements, the good welding technology performance is obtained, and the requirements for producing materials for oil and gas pipelines are met.

Description

technical field [0001] The invention relates to the field of metal smelting, in particular to an acid corrosion-resistant X70MS pipeline steel hot-rolled coil and a manufacturing method thereof. Background technique [0002] Acid-resistant pipeline steel is mainly used to transport oil and gas pipelines rich in acidic media. The main demand is for export and oil and gas field gathering and transportation pipelines in southwest China and other places. With the increase of oil and gas resource development, the quality of oil and gas in the world has been declining in recent years Trend, Cl in oil and gas - , SO 4 2- iso-salt content and CO 2 The content of acidic substances such as sulfide and sulfide increases. At the same time, the application of ultra-large pipe diameter and high-pressure conveying technology increases the erosion corrosion and corrosion fatigue of pipeline steel fluid, which puts forward higher requirements for the strength and corrosion resistance of p...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
25 Dec 2018
Publication
CN109082601A
IPC
C22C38/04; C22C38/02; C22C38/06; C22C38/44; C22C38/50; C22C38/48; C22C38/46; C21D8/02; C22C33/06
CPC
C22C38/04; C21D8/0226; C22C33/06; C22C38/02; C22C38/06; C22C38/44; C22C38/46; C22C38/48
Inventors
文小明; 赵迪