Embodiment Construction
[0026] 1. Preparation of water-based IPN emulsion:
[0027] Mix according to the mass ratio in the following table to prepare each water-based IPN emulsion:
[0028]
[0029] 2. Preparation of coating:
[0030] (1) According to the mass parts in the following table, first mix the water-based IPN emulsion, dispersant and defoamer, add fillers and other additives during stirring, stir at 1000-2000 rpm, disperse for 1-4 hours, Obtain a homogeneous mixture 1.
[0031] (2) Slowly add the thickener and deionized water into the above-mentioned mixture 1, stir for 1-20 minutes at a stirring speed of 800-1500 rpm, and obtain a uniform mixture 2.
[0032] (3) Filter the mixed material 2, and take the filtered material, that is, the paint.
[0033]
[0034] 3. Coating application and performance appraisal results:
[0035] The samples of the above embodiments have excellent noise reduction and shock absorption properties, and they have relatively high composite loss factors in ...