[0015] Embodiment one: by weight percentage bentonite 52%, wood flour 46%, carboxymethyl cellulose 2% are prepared raw materials, and wood flour can be pulverized into finer than 30 mesh granular things through pulverizing equipment with sawdust, wood shavings, and equipment can select feed, food etc. for use The pulverizer in the industry; bentonite can be processed into a fine powder finer than 200 mesh by Raymond machine or other machinery. Take 12% of bentonite and 28% of wood powder in the above raw materials and mix them evenly through mixing equipment. According to different shapes, use equipment such as screw extruder, feed machine, and turntable ball forming machine to process them into cat litter bases of different shapes. The inner core; then, the bentonite, wood powder and carboxymethyl cellulose used for producing the surface covering mixture are uniformly mixed in a mixer in a ratio of 40:18:2 to make the surface covering mixture. Put the cat litter matrix into t...
Embodiment 2
[0016] Embodiment two: prepare materials by weight percentage wood powder 35%, bentonite 60%, bamboo powder 5%, bamboo powder is used to improve product appearance, bentonite 15%, wood powder 35% are prepared matrix core by example one method, get bentonite 45%, bamboo powder 5% make the surface covering mixture and stir evenly to make the surface covering mixture, then make the specific gravity by the method described in Example 1 as 0.46, and the consumption of 20 milliliters of 3% salt water is 23 grams, consolidated Cat litter for pets with a compressive strength of 750 grams. In this example, because no bonding material is used, the amount of clay is increased, so the specific gravity and amount are increased, and the compressive strength is reduced.
Embodiment 3
[0017] Embodiment three: by weight percentage wood powder 42%, bentonite 35%, water-absorbing agent 14%, carboxymethyl starch 9% are prepared materials, first get wood powder 42%, bentonite 15%, superabsorbent resin 14% by weight percentage, put Add appropriate amount of water to wood flour and bentonite and mix evenly, add super absorbent resin to mix evenly and process it into matrix core; then take 20% bentonite and 9% carboxymethyl starch and mix evenly as surface covering mixture, then follow the method of Example 1 The specific gravity of the prepared cat litter is 0.37, the consumption of 20 ml of 3% salt water is about 7 grams, and the compressive strength of the consolidated matter is about 700 grams.
[0018] According to the needs of the market, the present invention can be made into cat litter products of various shapes and sizes. The basic shapes are spherical, cylindrical, flake and irregular granular, etc. The particle size is basically divided into the following...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com