A processing method and leather technology, applied in the field of leather and leather products and their processing, can solve problems such as crashes, quality and effect discounts, and difficulty for consumers to reflect individuality, etc., to achieve the effect of improving quality and enriching color difference
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0036] A leather processing method, comprising the following steps: liming, deliming and pickling, tanning, retanning and dyeing, stretch board drying, finishing, varnish spraying, ironing, softening, etc. for degreased and dehaired raw hides.
[0037] In the above-mentioned process, the described finishing process is as follows:
[0038] Raw material formula of oil wax liquid and cracking liquid:
[0039] The raw material composition (% by weight) of the oily wax liquid: 10% of vegetable oil, 50% of paraffin, 10% of penetrating agent whose active ingredient is alkylphenol polyoxyethylene ether, and 30% of water.
[0040] The raw material composition of the cracking liquid (% by weight): 20% of the cracking liquid, 40% of casein, 5% of penetrating agent whose active ingredient is alkylphenol polyoxyethylene ether, 5% of brightening agent, and 30% of water.
[0041] Finishing process:
[0042] Manually add the above-mentioned oil and wax solution to the back of the dry skin t...
Embodiment 2
[0047] In embodiment 2, the leather processing method is basically the same as in embodiment 1, and the raw material formulations of the oil wax liquid and cracking liquid are changed.
[0048] Raw material formula of oil wax liquid and cracking liquid:
[0049] The raw material composition (% by weight) of the oil wax liquid: 15% of animal oil, 45% of polyethylene wax, 10% of penetrating agent whose active ingredient is aliphatic polyurethane emulsion, and 30% of water.
[0050] The raw material composition of the cracking fluid (% by weight): 25% of the cracking fluid, 35% of casein, 6% of penetrating agent of aliphatic polyurethane emulsion, 4% of brightening agent, and 30% of water.
[0051] Finishing process:
[0052] Manually add the above-mentioned oil and wax solution to the back of the dry skin that has been dried with a stretching plate on the table, allowing it to naturally penetrate to the front of the dry skin until oil and wax stains appear on the front of the dry...
Embodiment 3
[0057] In embodiment 3, the leather processing method is basically the same as in embodiment 1, and the raw material formulations of the oil wax liquid and cracking liquid are changed.
[0058] Raw material formula of oil wax liquid and cracking liquid:
[0059] The raw material composition (% by weight) of the oil wax liquid: 8% of animal oil, 50% of Fischer-Tropsch wax, 12% of penetrating agent whose active ingredient is dioctyl sulfosuccinate sodium salt, and 30% of water.
[0060] The raw material composition of the cracking liquid (% by weight): 15% of the cracking liquid, 45% of casein, 5% of penetrating agent whose active ingredient is dioctyl sulfosuccinate sodium salt, 5% of brightening agent, and 30% of water.
[0061] Finishing process:
[0062] Manually add the above-mentioned oil and wax solution to the back of the dry skin that has been dried with a stretching plate on the table, allowing it to naturally penetrate to the front of the dry skin until oil and wax s...