Production method for novel composite material textile spool paper
A composite material and production method technology, applied in the field of papermaking, can solve the problems of not being able to meet the requirements of bobbin paper, general strength, etc., and achieve the effects of novel proportioning, strong tensile strength, and protection of ecological resources
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] The production method of the new composite bobbin paper is to mix straw pulp, wood pulp, waste paper pulp and bamboo pulp with a fiber length of 1.5mm in a mass ratio of 1:1:2.5:5, add water to dilute, and then add the pulp 6% of the total weight of papermaking additives and fillers, after dilution, go on the machine to produce bobbin paper. In order to increase the strength and prevent the bobbin paper from getting moldy, the papermaking additives contain antioxidants, water resistance agents and reinforcing agents. The mass ratio is 1: 1:2.
Embodiment 2
[0015] The production method of the new composite bobbin paper is to mix straw pulp, wood pulp, waste paper pulp and bamboo pulp with a fiber length of 2.0mm in a mass ratio of 1:1:2:5.5, add water to dilute, and then add the pulp 6.5% of the total weight of papermaking additives and fillers, after dilution, go on the machine to produce bobbin paper. In order to increase the strength and prevent the bobbin paper from getting moldy, the papermaking additives contain antioxidants, water resistance agents and reinforcing agents. The mass ratio is 1: 1:2.
Embodiment 3
[0017] The production method of the new composite bobbin paper is to mix straw pulp, wood pulp, waste paper pulp and bamboo pulp with a fiber length of 2.5mm in a mass ratio of 1:1:3:6, add water to dilute, and then add the pulp 7% of the total weight of papermaking additives and fillers, after dilution, go on the machine to produce bobbin paper. In order to increase the strength and prevent the bobbin paper from getting moldy, the papermaking additives contain antioxidants, water resistance agents and reinforcing agents. The mass ratio is 1: 1:2.
PUM
| Property | Measurement | Unit |
|---|---|---|
| Fiber length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More 