Double-face leather fatting agent and preparation method thereof

A fatliquoring agent and wool leather technology, applied in the field of wool leather fatliquor and its preparation, can solve the problems of the fatliquoring agent absorption effect (low absorption rate, waste of raw materials, environmental pollution, increasing the amount of the fatliquor, etc.) Smooth and moist hand, light leather color, good fatliquoring effect

Active Publication Date: 2015-01-21
BEIJING FANBO CHEM
View PDF3 Cites 7 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

At present, the common fatliquors mostly start from the feel of the fatliquored leather board, and seldom pay attention to the absorption effect of the fur to the fatliquor (the absorption rate is low). In order to achieve a good fatliquoring effect, it is necessary to Increasing the amount of fatliquoring agent will inevitably lead to waste of raw materials and environmental pollution

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Double-face leather fatting agent and preparation method thereof
  • Double-face leather fatting agent and preparation method thereof

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0059] The wool leather fatliquoring agent provided by the embodiment of the present invention, according to parts by weight, its components include: 70 parts of neutral oil and 15 parts of emulsifier;

[0060] In neutral oil, by weight percentage: 8% chlorinated alkanes, 70% epoxidized oil esters, 22% higher fatty acids and higher fatty alcohols;

[0061] Chlorinated alkanes: composed of 25%-32% chlorine-containing synthetic cowshoe oil and 42-degree chlorinated paraffin in a weight ratio of 4:1; epoxidized oil esters: composed of epoxidized fatty acid methyl ester and epoxidized three Fatty acid glycerides are composed at a weight ratio of 4:1; higher fatty acids and higher fatty alcohols are equal in weight;

[0062] In the emulsifier, by weight percentage, it includes 50% of amphoteric surfactant, 20% of nonionic hydrophilic surfactant, and 30% of nonionic lipophilic surfactant;

[0063] More specifically, the higher fatty acid is: n-dodecanoic acid;

[0064] Higher fatt...

Embodiment 2

[0078] The wool leather fatliquoring agent provided by the embodiment of the present invention, according to parts by weight, its components include: 85 parts of neutral oil and 30 parts of emulsifier;

[0079] In neutral oil, by weight percentage: chlorinated alkanes 12%, epoxidized oil esters 65%, higher fatty acids and higher fatty alcohols 23%;

[0080] Chlorinated alkanes: composed of synthetic cowshoe oil containing 25%-32% chlorine and 42-degree chlorinated paraffin in a weight ratio of 7:3;

[0081] Epoxidized oil ester: composed of epoxidized fatty acid methyl ester and epoxidized triglyceride fatty acid in a weight ratio of 7:3;

[0082] Higher fatty acid and higher fatty alcohol equal weight;

[0083] In the emulsifier, by weight percentage, it includes 70% of amphoteric surfactant, 10% of nonionic hydrophilic surfactant, and 30% of nonionic lipophilic surfactant;

[0084] More specifically, the higher fatty acid is: n-dodecanoic acid;

[0085] Higher fatty alcoh...

experiment example 3

[0099] The wool leather fatliquoring agent provided by the embodiment of the present invention, in parts by weight, its components include: 77 parts of neutral oil and 23 parts of emulsifier;

[0100] In neutral oil, by weight percentage: chlorinated alkanes 8%, epoxidized oil esters 75%, higher fatty acids and higher fatty alcohols 17%;

[0101] Chlorinated alkanes: composed of synthetic cowshoe oil containing 25%-32% chlorine and 42-degree chlorinated paraffin in a weight ratio of 9:1;

[0102] Epoxidized oil ester: composed of epoxidized fatty acid methyl ester and epoxidized triglyceride fatty acid in a weight ratio of 9:1;

[0103] Higher fatty acid and higher fatty alcohol equal weight;

[0104] In the emulsifier, by weight percentage, it includes 60% of amphoteric surfactant, 15% of nonionic hydrophilic surfactant, and 25% of nonionic lipophilic surfactant;

[0105] More specifically, the higher fatty acid is: n-hexadecanoic acid;

[0106] Higher fatty alcohol: n-hex...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention provides a double-face leather fatting agent and a preparation method thereof, and belongs to the technical field of double-face leather processing. The double-face leather fatting agent comprises the following components in parts by weight: 70-85 parts of neutral oil and 15-30 parts of emulsifier, wherein the neutral oil comprises chlorinated alkane, epoxidized oil ester, higher aliphatic acid and higher aliphatic alcohol; the emulsifier comprises an ampholytic surfactant, a nonionic hydrophilic surfactant and a nonionic lipophilic surfactant. After the fatting agent provided by the invention is applied to the main oiling process of double-face leather, the absorptivity of the fatting agent can be up to 93-96%, the leather board is flexible, full, strong in forming sense, shallow in color and smooth and moist in hand feel, good fatting effect is provided, and the defect that the common fatting agents in the prior art are low in adsorptivity to cause waste and environment pollution is overcome.

Description

technical field [0001] The invention relates to the technical field of wool leather processing, in particular to a wool leather fatliquoring agent and a preparation method thereof. Background technique [0002] The fatliquoring agent for fur leather requires that after oiling, the leather board is soft and has a sponge-like foaming feeling, the flesh surface of the leather board feels smooth, has a certain degree of moisture retention, the color of the leather board is light, and has good light resistance. [0003] During the fatliquoring process of fur leather, in order to reduce the pollution to the environment, the fatliquoring agent should be absorbed by the leather plate as much as possible, so that its residual amount in the fatliquoring bath is small. At present, the common fatliquors mostly start from the feel of the fatliquored leather board, and seldom pay attention to the absorption effect of the fur to the fatliquor (the absorption rate is low). In order to achie...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C14C9/02
CPCC14C9/02
Inventor 郑超斌郑红超郝安生
Owner BEIJING FANBO CHEM
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products