[0017] The invention provides a decorative panel manufacturing process with gradient effect, comprising the following steps:
[0018] a. Select the substrate, plan the pattern area to be processed on the substrate according to the pattern shape that needs to be formed, and prepare the screen printing colored screen line, back cover and front dot film;
[0019] b. According to the needs of the printing effect, prepare the screen plate of the corresponding mesh;
[0020] c. Send the substrate into a semi-automatic screen printing machine, and print a dot layer composed of several regularly distributed colored dots on the back of the substrate by screen printing. The size of the colored dots in the dot layer is determined by the center in the pattern area Gradually increase towards the edge, the screen line angle of the colored dots is 40 degrees, after printing, send it to the electric heating dryer, and dry it for 30 minutes at a temperature of 50 degrees Celsius;
[0021] d. ...
Embodiment 2
[0024] A manufacturing process for a decorative panel with a gradient effect, comprising the following steps:
[0025] a. Select the substrate, plan the pattern area to be processed on the substrate according to the pattern shape that needs to be formed, and prepare the screen printing colored screen line, back cover and front dot film;
[0026] b. According to the needs of the printing effect, prepare the screen plate of the corresponding mesh;
[0027] c. Send the substrate into a semi-automatic screen printing machine, and print a dot layer composed of several regularly distributed colored dots on the back of the substrate by screen printing. The size of the colored dots in the dot layer is determined by the center in the pattern area Gradually increase towards the edge, the screen line angle of the colored dots is 50 degrees, after printing, send it to the electric heating dryer, and dry it for 20 minutes at a temperature of 55 degrees Celsius;
[0028] d. Send the substr...
Embodiment 3
[0031] A manufacturing process for a decorative panel with a gradient effect, comprising the following steps:
[0032] a. Select the substrate, plan the pattern area to be processed on the substrate according to the pattern shape that needs to be formed, and prepare the screen printing colored screen line, back cover and front dot film;
[0033] b. According to the needs of the printing effect, prepare the screen plate of the corresponding mesh;
[0034] c. Send the substrate into a semi-automatic screen printing machine, and print a dot layer composed of several regularly distributed colored dots on the back of the substrate by screen printing. The size of the colored dots in the dot layer is determined by the center in the pattern area Gradually increase towards the edge, the screen line angle of the colored dots is 45 degrees, after printing, send it to the electric heating dryer, and dry it for 25 minutes at a temperature of 52 degrees Celsius;
[0035] d. Send the substr...