Polymethyl methacrylate (PMMA) decorative board printed with three-dimensional image and printing process of PMMA decorative board
A three-dimensional, decorative board technology, used in printing technology, printing of special varieties of printed matter, decorative arts, etc., can solve the problems of inability to perform local processing, dizziness, etc., and achieve flexible and vivid pattern visual effects, simple process, and external dimensions. flexible effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] Example 1: Production of on-hook panels for air conditioners
[0030] (1) Select a substrate 2 made of polymethyl methacrylate (PMMA) with a thickness of 1.5mm, and plan a pattern area for forming a three-dimensional image on the substrate 2 according to the pattern shape to be formed. The substrate 2 is sent into a semi-automatic screen printing machine, and a dot layer 3 composed of several regularly distributed colored dots is printed on the back of the substrate 2 by screen printing. The size of the colored dots in the dot layer 3 is determined by The center gradually increases toward the edge, and the angle of the screen line of the colored dots is 45°. After the printing is completed, it is sent to an electric heating dryer and dried for 20 minutes at a temperature of 50°C, and the printing of the dot layer 3 is completed;
[0031] (2) The printed substrate 2 of the colored dot layer 3 is sent to a semi-automatic screen printing machine, using a 200-mesh screen, a...
Embodiment 2
[0034] Example 2: Production of air-conditioning cabinet panels
[0035] (1) Select a substrate 2 made of polymethyl methacrylate (PMMA) material with a thickness of 3mm, and plan a pattern area for forming a three-dimensional image on the substrate 2 according to the required pattern shape, and place the substrate 2. Send it into a semi-automatic screen printing machine, and print a dot layer 3 composed of several regularly distributed colored dots on the back of the substrate 2 by screen printing. The size of the colored dots in the dot layer 3 is determined by the center Gradually increase towards the edge, the screen line angle of the colored dots is 45°, after the printing is completed, send it to the electric heating dryer, and dry it for 25 minutes at a temperature of 52°C, and the printing of the dot layer 3 is completed;
[0036] (2) The printed substrate 2 of the colored dot layer 3 is sent to a semi-automatic screen printing machine, using a 300-mesh screen, and st...
Embodiment 3
[0039]Example 3: Production of refrigerator panels
[0040] (1) Select a substrate 2 made of polymethyl methacrylate (PMMA) material with a thickness of 5mm, and plan a pattern area for forming a three-dimensional image on the substrate 2 according to the required pattern shape. 2. Send it into a semi-automatic screen printing machine, and print a dot layer 3 composed of several regularly distributed colored dots on the back of the substrate 2 by screen printing. The size of the colored dots in the dot layer 3 is determined by the center Gradually increase towards the edge, the screen line angle of the colored dots is 45°, after the printing is completed, send it to the electric heating dryer, and dry it at a temperature of 55°C for 30 minutes, and the printing of the dot layer 3 is completed;
[0041] (2) The printed substrate 2 of the colored dot layer 3 is sent to a semi-automatic screen printing machine, using a 200-mesh screen, and still printing the reflective coating pr...