A nanoemulsion and porous media technology, applied in the direction of measuring devices, flow characteristics, and preparation of test samples, can solve problems such as difficult to reproduce, irreproducible, and affect application effects, so as to reduce operational errors and particle size changes , to ensure the effect of uniformity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0055] The nanoemulsion comprises the following components based on 100 parts by weight: 20 parts of liquid paraffin, 4.88 parts of nonionic surfactant Span 20, 5.12 parts of Tween 20, and the balance is deionized water. The mechanical stirring rate is 750 rpm, the electromagnetic stirring rate is 100 rpm, the temperature is 25°C, the rate of the first injection pump is 0.5mL / min, and the rate of the fourth injection pump is 9.99mL / min. Put the rock core with a permeability of 253mD into the core holder, control the confining pressure to 8MPa, collect the change of pressure through the data acquisition system, and obtain the flow of the nanoemulsion in the porous medium. The particle size of the nanoemulsion under different conditions was measured and characterized by a nanometer laser particle size analyzer.
Embodiment 2
[0057] The nanoemulsion comprises the following components based on 100 parts by weight: 20 parts of liquid paraffin, 4.88 parts of nonionic surfactant Span 20, 5.12 parts of Tween 20, and the balance is deionized water. The mechanical stirring rate was 750 rpm. The electromagnetic stirring rate is 1000 rpm, the temperature is 25°C, the speed of the first sampling pump is 0.5mL / min, and the speed of the fourth sampling pump is 9.99mL / min. Put the rock core with a permeability of 253mD into the core holder, control the confining pressure to 8MPa, collect the change of pressure through the data acquisition system, and obtain the flow of the nanoemulsion at different core permeability.
Embodiment 3
[0059] The nanoemulsion comprises the following components based on 100 parts by weight: 20 parts of liquid paraffin, 4.88 parts of nonionic surfactant Span 20, 5.12 parts of Tween 20, and the balance is deionized water. The mechanical stirring rate is 750 rpm, the electromagnetic stirring rate is 100 rpm, the temperature is 25°C, the rate of the first injection pump is 0.5mL / min, and the rate of the fourth injection pump is 9.99mL / min. Put the core with a permeability of 136mD into the core holder, control the confining pressure to 8MPa, collect the change of pressure through the data acquisition system, and obtain the flow of the nanoemulsion in the porous medium.
PUM
Property | Measurement | Unit |
---|---|---|
thermal resistance | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com