Leveling modified guitar musical instrument nitryl paint formula and manufacturing method thereof

A technology of polyether modification and nitrocellulose, which is applied in coatings, polyester coatings, etc., can solve the problems of poor leveling of nitro coatings, and achieve the effect of improving leveling

CN106811025AInactive Publication Date: 2017-06-09闫斐斐
0 Cites 0 Cited by

Patent Information

Authority / Receiving Office
CN · China
Current Assignee / Owner
Publication Date
2017-06-09
Estimated Expiration
Not applicable · inactive patent
Patent Text Reader

Abstract

The invention provides the technical scheme of a formula for solving the problem of poor leveling effect of guitar musical instrument nitryl paint and a manufacturing method thereof. The paint is prepared from the following ingredients in percentage by weight: 10 to 15 percent of ethyl acetate, 10 to 15 percent of n-butyl acetate, 5 to 10 percent of isopropanol, 3 to 5 percent of propylene glycol monomethyl ether acetate, 20 to 25 percent of 1 / 16 second nitrocellulose, 1 to 5 percent of efficient extinction powder, 20 to 30 percent of 70-percent alkyd resin polymers, 1 to 5 percent of non-extinction wax liquid and 0.1 to 1 percent of polyether modified polydimethyl siloxane.
Need to check novelty before this filing date? Find Prior Art

Description

technical field

[0001] The invention relates to the field of chemical paint manufacturing, in particular to a formula for improving the leveling performance of nitro paint for guitar musical instruments and a manufacturing method thereof. Background technique

[0002] Currently, nitro lacquers for guitar instruments on the market generally have problems of high viscosity and unsatisfactory leveling effect, which can easily lead to problems such as "orange peel" and protruding Bernard swirls that affect the final effect of guitar instrument coatings and affect the quality of guitar instruments. beautiful. Contents of the invention

[0003] The invention solves the problem of poor leveling of the existing nitro paint for guitar musical instruments, and invents a formula improved by using a leveling agent and a manufacturing method thereof.

[0004] The technical scheme of the present invention is, a kind of formula and its manufacture method that solves the poor leveling of...

Examples

Embodiment Construction

[0011] 15 kg of ethyl acetate, 15 kg of n-butyl acetate, 5 kg of isopropanol, 5 kg of propylene glycol methyl ether acetate, 20 kg of 1 / 16 second nitrocellulose, 2 kg of high-efficiency matting powder, 70% alkyd resin polymer 30 kg, 5 kg of matt wax slurry, and 0.1 kg of polyether modified polydimethylsiloxane. Add ethyl acetate, n-butyl acetate, isopropanol, propylene glycol methyl ether acetate, and 1 / 16 second nitrocellulose in sequence, and continue stirring for 30 minutes. After the nitrocellulose is completely dissolved, add 70% alkyd resin polymer, Continue stirring for 30 minutes, and finally add high-efficiency matting powder, matting wax paste, polyether modified polydimethylsiloxane, and stir for 10 minutes.