Welding method of stainless steel plates
A welding method, stainless steel technology, applied in welding equipment, laser welding equipment, welding/welding/cutting items, etc., can solve the problem of not using laser welding stainless steel plate, etc., to achieve the effect of ensuring mechanical properties
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2018-10-26
- Estimated Expiration
- Not applicable · inactive patent
Abstract
Description
technical field
[0001] The invention relates to the field of welding technology, in particular to a welding method for stainless steel plates. Background technique
[0002] Laser is a kind of electromagnetic wave with good monochromaticity, good directionality, high brightness and good coherence due to stimulated radiation. Due to the above remarkable characteristics, the energy of the laser beam can be converged to a relatively small point , so that the power density on the workpiece can reach more than 107W / cm2. The incident power density of this order can vaporize the metal in the heating zone in a very short time, thus forming a small hole in the liquid molten pool, called the keyhole. The beam can directly enter the keyhole, and through the heat transfer of the keyhole, a larger welding penetration can be obtained. The essence of laser welding is the process of interaction between laser and non-transparent substances. This process is extremely complicated and is a qua...
Examples
Embodiment Construction
[0036] Below, the substantive features and advantages of the present invention will be further described in conjunction with examples, but the present invention is not limited to the listed examples.
[0037] A welding method for stainless steel plates provided by the invention comprises:
[0038] 1) Pretreatment and cleaning of the two stainless steel plates to be welded;
[0039] 2) Preheat the stainless steel plate to reduce the maximum hardness of the whole plate, and the preheating temperature is 250-350°C;
[0040] 3) Input the workpiece information of the two stainless steel plates to be welded, overlap the welding parts of the two stainless steel plates to be welded, and determine the welding path;
[0041] 4) Carry out chamfering and turning on the weld joint along the welding path, and the chamfering angle is 45°;
[0042] 5) Use a fiber laser to perform penetration welding on the chamfer, set the first laser power to 3.60-3.75KW, the second laser power to 4.35-4.7...