A lithium-ion battery and processing technology, applied in battery electrodes, electrode manufacturing, circuits, etc., can solve problems such as increased power consumption, powder removal, and increased production costs, to improve wetting effect, enhance liquid absorption capacity, increase The effect of adhesion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0033] Dissolve PVDF in NMP to make PVDF glue with a solid content of 6.0%, and coat it on the unrolled graphite negative electrode sheet. The thickness of the PVDF glue layer is 1-3 μm. The coating method is as follows: figure 1 , figure 2 , Both sides of the current collector 1 are the pole piece coating 2, and the outer surface of the pole piece coating 2 is coated with a protective layer 3, and the protective layer 3 is an adhesive layer or a ceramic coating.
Embodiment 2
[0035] Dissolve PVDF in NMP to make PVDF glue, then add ceramic powder to make ceramic slurry, wherein the mass ratio of PVDF to ceramic is 3:1, and the solid content of the slurry is 20%. On the roll-pressed positive electrode sheet, the thickness of the PVDF+ceramic coating is 5-8 μm, and the coating method is as follows: figure 1 , figure 2 .
Embodiment 3
[0037] Dissolve CMC in deionized water to make CMC glue with a solid content of 1.5%, and coat it on the non-rolled silicon carbon negative electrode sheet. The thickness of the CMC glue layer is 10-12 μm. The coating method is as follows: figure 1 , figure 2 .
PUM
| Property | Measurement | Unit |
|---|---|---|
| Thickness | aaaaa | aaaaa |
| Thickness | aaaaa | aaaaa |
| Thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More 