A technology of ultrasonic coupling agent and bactericide, which is applied in the field of clinical medical testing, can solve the problems that cannot meet the detection of cavities, mucous membranes and incomplete skin, low irritation, high safety, etc., and achieve low cost of raw materials and low irritation , high safety effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0037] The ultrasonic coupling agent of the present embodiment, its raw material is made up of each component of following parts by weight:
[0038] Silver nitrate 0.2g
[0039] Hydroxyethylcellulose 25.0g
[0040] Amino Acid Zinc 5.0g
[0041] Sodium polyphosphate 5.0g
[0042] Allantoin 1.0g
[0043] Deionized water 963.8g
[0044] The total amount is 1000g
[0045] The preparation method of the present embodiment ultrasonic coupling agent, its steps are as follows:
[0046] Dissolve amino acid zinc, allantoin and sodium polyphosphate in deionized water, add hydroxyethyl cellulose, stir until the liquid is transparent, add silver nitrate solution, stir and mix well, adjust the pH of the whole system to 5-7 with NaOH , vacuum degassed, canned.
Embodiment 2
[0048] The ultrasonic coupling agent of the present embodiment, its raw material is made up of each component of following parts by weight:
[0049] Silver nitrate 0.2g
[0050] Carbomer 5.0g
[0051] Zinc acetate 5.0g
[0052] Sodium polyphosphate 5.0g
[0053] Allantoin 1.0g
[0054] Deionized water 983.8g
[0055] The total amount is 1000g
[0056] The preparation method of the present embodiment ultrasonic coupling agent, its steps are as follows:
[0057] Dissolve zinc acetate, allantoin, and sodium polyphosphate in deionized water in a sugar porcelain stirring pot, add carbomer, stir, and when the liquid is transparent, add silver nitrate solution, stir and mix well, add an appropriate amount of NaOH solution to adjust the pH and viscosity, control the pH of the whole system to 5-7, vacuum degassing, and canning.
Embodiment 3
[0059] The ultrasonic coupling agent of the present embodiment, its raw material is made up of each component of following parts by weight:
[0060]Nano Silver Colloid 0.5g
[0061] Carbomer 5.0g
[0062] Zinc acetate 5.0g
[0063] Sodium polyphosphate 5.0g
[0064] Allantoin 1.0g
[0065] Deionized water 983.5g
[0066] The total amount is 1000g
[0067] The preparation method of the present embodiment ultrasonic coupling agent, its steps are as follows:
[0068] Add part of deionized water to zinc acetate, allantoin and sodium polyphosphate in the sugar porcelain stirring pot, then add nano-silver colloid dispersed in advance, stir to dissolve, then add carbomer, make up the remaining amount of deionized water, Homogeneously disperse, add appropriate amount of NaOH solution to adjust pH and viscosity, control the pH of the whole system to 5-7, vacuum degassing, and pack in cans.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com