Laminate flooring colorized solid sealing wax and preparation method thereof
A technology of strengthening wood floor and color, applied in chemical instruments and methods, other chemical processes, etc., can solve the problems of uneven surface color, blackened substrate at the floor splicing, unable to cover the substrate at the floor lock, etc. Improve overall aesthetics and color uniformity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0024] The preparation method of the colored solid sealing wax for laminate flooring is as follows: Weigh the required raw materials in proportion, melt and mix the raw materials, and then cool. The steps of melting and mixing are as follows:
[0025] (A) dissolving the surface modifier in 5-20 times the weight of ethanol, then spraying it on the surface of the powdery polymer material, stirring evenly; then drying it in a vacuum oven at 50°C for 3-5 hours;
[0026] (B) heating and melting the polymer material obtained in step A, and mixing it with the organic pigment;
[0027] (C) heating, melting and mixing the material obtained in step B with paraffin.
Embodiment 1
[0029] The components used in this embodiment are as follows:
[0030] Microcrystalline Wax 70%, Polyethylene Wax 22%,
[0031] Toluidine Red 4%, Span-60 4%.
[0032] Preparation Process:
[0033] (A) Dissolve Span-60 in 10 times the weight of ethanol, then spray on the surface of the powdery polyethylene wax, and stir while dispersing; then place the polyethylene wax after the surfactant treatment at 50°C Dry in a vacuum oven for 4 hours;
[0034] (B) Melt the dried polyethylene wax at 120°C, add toluidine red in the molten state, stir and mix evenly;
[0035] (C) In molten state, add paraffin and stir well.
[0036] (D) After cooling, the colored solid sealing wax for laminate flooring is obtained.
Embodiment 2
[0038] The components used in this embodiment are as follows:
[0039] Microcrystalline Wax 85%, Polyethylene Wax 10%,
[0040] Phthalo Blue 2%, Span-60 3%.
[0041] In the preparation process (A), dry in a vacuum oven for 5 hours, and the rest are the same as in Example 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology