[0022] Sodium caseinate (SC) and transglutaminase (MTG, specific activity 200U / g) were dissolved in 0.1M, pH 7.0 Tris-HCl buffer to obtain a reinforcement solution, in which the mass concentration of SC was 3%, MTG enzyme Vitality / SC mass=30U / g; use the brushing method to apply the reinforcement solution evenly on the surface of the simulated ancient silk fabric sample, every 10cm 2 The surface of the textile was coated with 1mL of reinforcement solution, and then the sample was incubated at 25°C for 3 hours and then taken out for analysis. The tensile strength was 1.62N, and the color difference ΔE = 1.22.
[0023]
Embodiment 2
[0025] Dissolve sodium caseinate (SC) and transglutaminase (MTG, specific activity 200U / g) in 0.1M, pH 7.0 Tris-HCl buffer to obtain a reinforcement solution, in which the mass concentration of SC is 0.5%, and MTG enzyme Vitality / SC mass=20U / g; use the brushing method to apply the reinforcement solution evenly on the surface of the simulated ancient silk fabric sample, every 10cm 2 The surface of the textile was coated with 1mL of reinforcement solution, and then the sample was incubated at 37°C for 1 hour and then taken out for analysis. The tensile strength was 1.54N, and the color difference ΔE = 0.60.
[0026]
Embodiment 3
[0028] Sodium caseinate (SC) and transglutaminase (MTG, specific activity 200U / g) were dissolved in 0.1M, pH 7.0 Tris-HCl buffer to obtain a reinforcement solution, in which the mass concentration of SC was 2%, MTG enzyme Vitality / SC mass=30U / g; use the brushing method to apply the reinforcement solution evenly on the surface of the simulated ancient silk fabric sample, every 10cm 2 The surface of the textile was coated with 1mL of reinforcement solution, and then the sample was taken out for analysis after being incubated at 50°C for 3 hours. The tensile strength was 2.62N, and the color difference ΔE = 0.92.
[0029]
PUM
Property | Measurement | Unit |
---|---|---|
chromatic aberration | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com