[0026] like figure 1 As shown, the metal watchband edge sealing mechanism disclosed by the present invention includes a belt grain 1, a watch grain 2, a first sleeve 3 and a first pin 4, and belt grain holes 11 are provided at both ends of the belt grain 1, The inside of the watch grain 2 is provided with two counterbores 21, the first sleeve 3 is a cylindrical body with a C-shaped cross section, the first insertion pin 4 is a columnar body, and the first sleeve 3 is cylindrical. Inserted into the grain hole 11 , one end of the first pin 4 is inserted into the counterbore 21 on the watch grain 2 , and the other end is inserted into the first sleeve 3 .
[0027] The cross-sectional diameter of the first sleeve 3 is smaller than that of the inside of the first pin 4 , and the cross-sectional diameter of the particle-carrying hole 11 is larger than the cross-sectional diameter of the first sleeve 3 .
[0028] The specific installation process of this embodiment is: insert the fi...
no. 2 example
[0030] like figure 2 As shown, the edge banding mechanism of this embodiment includes, in addition to the belt grain 1 and the first sleeve 3 in the first embodiment, a second grain 6, a second pin 5, and two grains of the second grain 6. There is a surface hole 25 on the side, and the second insertion pin 5 is inserted into the surface hole 25 and fixed by laser spot welding. The second insertion pin 5 protrudes on the outside of the surface hole 25 The part is ground and smoothed, the first sleeve 3 is inserted into the particle-carrying hole 11 , and the second pin 5 is inserted into the first sleeve 3 .
[0031] The specific installation process of this embodiment is as follows: insert the second pins 5 on the left and right sides into the through holes 25 of the second watch grain 6, and carry out laser spot welding and welding firmly, and then insert the second pins 5 The part protruding from the outer surface of the watch grain is polished smooth, insert the second pi...
no. 3 example
[0033] like image 3 As mentioned above, the edge banding mechanism of this embodiment also includes an inner sleeve 8, an outer sleeve 9 and a fourth pin 10 in addition to the belt grain 1 and the watch grain 2 in the first embodiment, and the inner sleeve 8 is set The outer casing 9 is arranged on the upper part of the counterbore 21 and closely fits with the counterbore 21. The cross-sectional diameter of the inner casing 8 is Smaller than the cross-sectional diameter of the outer sleeve 9 , the fourth pin 10 passes through the pellet hole 11 of the pellet 1 , and is sequentially inserted into the outer sleeve 9 and the inner sleeve 8 .
[0034] The specific installation process of this embodiment is: press the inner sleeves 8 on the left and right sides into the counterbore 21 of the watch grain 2, and then press the outer sleeve 9 into the counterbore 21, wherein the inner sleeve The tube 8 is in clearance fit with the counterbore, the outer sleeve 9 is closely matched w...