Embodiment 1
[0032] A method for preparing a contact lens with a two-dimensional code, comprising:
[0033] 1) Raw material preparation
[0034] A. Mix 30 parts of hydrogel, 0.5 parts of emulsion stabilizer and 0.8 part of monomethyl fumarate sodium salt by weight, keep the temperature at 32°C, heat for 30 minutes, and then place it in infrared rays with a wavelength of 900nm for 30 minutes and placed in a microwave with a frequency of 800MHz for 20 minutes, the two are alternately carried out, and the cycle is 2 times to obtain the first mixture;
[0035] B. Mix 20 parts of silicon hydrogel and 0.5 part of glycerin by weight, and heat at 40°C for 30 minutes to obtain the second mixture;
[0036] C. Mix the first mixture with the second mixture, place it in a vacuum device with a vacuum degree of 0.05MPa, raise the temperature to 40°C at a heating rate of 2°C / min, and keep it warm for 30min. During the heat preservation process, keep the vacuum device at a speed of 600r / min rotation, th...
Embodiment 2
[0049] A method for preparing a contact lens with a two-dimensional code, comprising:
[0050] 1) Raw material preparation
[0051] A. Take 30 parts of hydrogel, 0.5 parts of emulsion stabilizer, and 0.8 parts of monomethyl fumarate sodium salt by weight, mix them, keep the temperature at 33°C, heat for 30 minutes, and then place them in infrared rays with a wavelength of 900nm for 30 minutes. and placed in a microwave with a frequency of 800MHz for 20 minutes, the two are alternately carried out, and the cycle is 2 times to obtain the first mixture;
[0052] B. Mix 20 parts of silicon hydrogel and 0.5 part of glycerin by weight, and heat at 43°C for 30 minutes to obtain the second mixture;
[0053] C. Mix the first mixture with the second mixture, place it in a vacuum device with a vacuum degree of 0.05MPa, raise the temperature to 44°C at a heating rate of 2°C / min, and keep it warm for 30min. During the heat preservation process, keep the vacuum device at a speed of 600r / ...
Embodiment 3
[0066] A method for preparing a contact lens with a two-dimensional code, comprising:
[0067] 1) Raw material preparation
[0068] A. Take 30 parts of hydrogel, 0.5 parts of emulsion stabilizer, and 0.8 parts of monomethyl fumarate sodium salt in parts by weight, keep the temperature at 35°C, heat for 30 minutes, and then place it in infrared rays with a wavelength of 900nm for 30 minutes. and placed in a microwave with a frequency of 800MHz for 20 minutes, the two are alternately carried out, and the cycle is 2 times to obtain the first mixture;
[0069] B. Mix 20 parts of silicon hydrogel and 0.5 part of glycerin by weight, and heat at 45°C for 30 minutes to obtain the second mixture;
[0070] C. Mix the first mixture with the second mixture, place it in a vacuum device with a vacuum degree of 0.05MPa, raise the temperature to 50°C at a heating rate of 2°C / min, and keep it warm for 30min. During the heat preservation process, keep the vacuum device at a speed of 600r / min...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com