Low-temperature reduction smelting method of stibium-containing compound

An antimony compound, low temperature technology, applied in the field of pyrometallurgy process, can solve the problems of antimony volatilization and oxidation loss, reduce production efficiency, low antimony direct yield, etc., and achieve the effects of reducing energy consumption, low production cost, and low labor intensity

Active Publication Date: 2016-11-09
CENT SOUTH UNIV
View PDF3 Cites 7 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Due to the use of reduced pulverized coal as a reducing agent, there are two problems: one is the high smelting temperature, in order to make the slagging components in the reduced coal slagging smoothly, the smelting temperature needs to be kept between 1100 and 1200 °C; the other is On the one hand, the volatilization loss of antimony is serious, and the volatilization and oxidation loss of antimony is serious at high temperature. The volatilization loss of antimony brought about by the two stages of drafting away and volatilization during the feeding process reaches between 35% and 50%, so the direct recovery rate of antimony is usually low, greatly Reduced production efficiency, these problems have been plagued by production enterprises

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Low-temperature reduction smelting method of stibium-containing compound

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0020] The antimony in the raw material antimony white is 83.50% by weight, and the starch used is wheat starch. Add 1000g antimony white and 75g wheat starch into the conical mixer at the same time, control the stirring speed at 30r / min and stir for 120min, after stirring and mixing, put the mixture into the melting pot, and use the indirect heating method of burning natural gas to maintain the temperature in the melting pot At 815°C, start stirring to maintain the rotation speed at 60r / min, and the metal antimony produced by smelting is discharged continuously, and the direct recovery rate of antimony reaches 91.8%.

Embodiment 2

[0022] The antimony in the raw material sodium pyroantimonate is 48.50% by weight, and the starch used is wheat starch. Add 1000g of sodium pyroantimonate and 80g of wheat starch into the conical mixer at the same time, control the stirring speed at 30r / min and stir for 120min, after stirring and mixing, put the mixture into the melting pot, and use the indirect heating method of burning natural gas to make the melting pot The temperature is maintained at 815°C, the stirring is started to maintain the rotation speed at 60r / min, the metal antimony produced by smelting is continuously discharged, and the direct recovery rate of antimony reaches 92.5%.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses a low-temperature reduction smelting method of a stibium-containing compound. The low-temperature reduction smelting method of the stibium-containing compound comprises the following steps: simultaneously adding the stibium-containing compound and starch into a conical mixer, stirring and mixing; continuously conveying the mixed material to an indirect heating smelting pot; then heating to the required temperature and smelting; and further treating produced stibium. Under the condition of indirect heating, the starch is used as a reducing agent, the purpose of producing the stibium by low-temperature reduction smelting of the stibium-containing compound is achieved, reduction smelting temperature is reduced to be 800-850 DEG C, and the direct recovery rate of the stibium reaches 90.0% or above.

Description

technical field [0001] The invention relates to a pyrometallurgical process in the field of nonferrous metallurgy, in particular to a pyrometallurgical method for low-temperature reduction smelting of antimony-containing compounds. Background technique [0002] Antimony is a silver-white non-ferrous metal that is brittle and has poor electrical and thermal conductivity. It is mainly used in alloys, military industry, flame retardants and glass industries. my country is the country with the largest antimony output in the world. In 2010, the world's antimony output was 167,000 tons, while China's antimony output reached 150,000 tons in 2010, accounting for more than 89% of the world's antimony output. my country's antimony resources and production All have irreplaceable advantages. Mineral raw materials for antimony smelting mainly include stibnite, antimony gold ore, brittle lead-antimony ore, etc. At the same time, the antimony-containing soot produced in the smelting proces...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C22B30/02
CPCC22B30/02
Inventor 刘伟锋傅新欣邓循博朱鹏春令红斌杨天足张杜超陈霖
Owner CENT SOUTH UNIV
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products