A wood lacquer, environmentally friendly technology, applied in the field of paint, can solve problems such as affecting the overall experience, user physical injury, falling off, etc., to enhance functionality and practicability, improve adaptability and viscosity, and good adhesion and adhesion. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] Prepare this environmentally friendly PE wood lacquer with fragrance through the following steps:
[0020] Step 1: Mix the film-forming substance, filler, solvent and additive in a ratio of 10:1:1:1.5 to obtain the main paint, and mix the main agent, blue water, white water, and thinner in a ratio of 100:2 : 2: 50 proportioning is mixed to obtain auxiliary paint, and lavender vegetable oil, defoamer and paint preservative are mixed with 1: 1: 1 proportioning to obtain additive;
[0021] Step 2: The auxiliary paint obtained after mixing the main agent, blue water, white water and thinner according to the ratio of 100:2:2:50, and lavender vegetable oil, defoamer and paint preservative are mixed in a ratio of 1:1 : The additive obtained after mixing in the proportioning ratio of 1 is fully mixed according to the proportioning ratio of 2:1;
[0022] Step 3: After fully mixing the film-forming substances, fillers, solvents and additives according to the ratio of 10:1:1:1.5,...
Embodiment 2
[0024] Prepare this environmentally friendly PE wood lacquer with fragrance through the following steps:
[0025] Step 1: Mix the film-forming substance, filler, solvent and auxiliary agent according to the ratio of 10:1:2:1.5 to obtain the main paint, and mix the main agent, blue water, white water and thinner according to the ratio of 100:2 : 4: 50 proportioning is mixed to obtain auxiliary paint, and lavender vegetable oil, defoamer and paint preservative are mixed with 1: 1: 2 proportioning to obtain additive;
[0026] Step 2: The auxiliary paint obtained after mixing the main agent, blue water, white water and thinner according to the ratio of 100:2:4:50 and lavender vegetable oil, defoamer and paint preservative are mixed in a ratio of 1:1 The additive obtained after mixing in the proportioning ratio of 2:2 is fully mixed according to the proportioning ratio of 3:1;
[0027] Step 3: After fully mixing the film-forming substances, fillers, solvents and additives accordin...
Embodiment 3
[0029] Prepare this environmentally friendly PE wood lacquer with fragrance through the following steps:
[0030] Step 1: Mix the film-forming substances, fillers, solvents and additives at a ratio of 10:2:1:2.5 to obtain the main paint, and mix the main agent, blue water, white water, and thinner at a ratio of 100:4 : 2: 50 proportioning is mixed to obtain auxiliary paint, and lavender vegetable oil, defoamer and paint preservative are mixed with 1: 2: 1 proportioning to obtain additive;
[0031] Step 2: The auxiliary paint obtained after mixing the main agent, blue water, white water and thinner according to the ratio of 100:4:2:50 and lavender vegetable oil, defoamer and paint preservative are mixed in a ratio of 1:2 The additive obtained after mixing in the proportioning ratio of 1:1 is fully mixed according to the proportioning ratio of 2:1.5;
[0032]Step 3: After fully mixing the film-forming substances, fillers, solvents and additives according to the ratio of 10:2:1:...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com