A composition and pigment technology, applied in the direction of pigment slurry, color measuring device, device for coating liquid on the surface, etc., can solve the problem of inability to accurately control, achieve small color difference, good ratio reproducibility, weather resistance and high stability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] Weigh 27.64 grams of PY42, 2.75 grams of PR101, 0.54 grams of PBK7, and 1000 grams of CSC-B base material. Mix the above materials evenly, and then apply the obtained composition on the substrate evenly and evenly by mechanical coating under the conditions of relative humidity of 50%±5% and room temperature of 23±2°C. It is metallic or non-metallic material. The wet film thickness of the coating is 250m, and then placed in a 50±2°C precision oven to dry for 3-4h to constant weight, take it out, cool to room temperature, and obtain the color characterization.
Embodiment 2
[0025] Weigh 27.0 grams of PY42, 2.75 grams of PR101, 0.54 grams of PBK7, and 1000 grams of CSC-C base material. Manufacturing process is with embodiment 1.
Embodiment 3
[0027] Weigh 28.3 grams of PY42, 2.75 grams of PR101, 0.54 grams of PBK7, and 1005 grams of CSC-C base material. Manufacturing process is with embodiment 1.