[0022] Example 1:
[0023] Weigh 0.05 grams of PBK7, 5.60 grams of PY138, 0.18 grams of PG7, and 1000 grams of CSC-A base material by weight. Mix and mix the above-mentioned raw materials uniformly, and then apply the mixed composition to the coated paper evenly and smoothly under the environmental conditions of 50%±5% relative humidity and 23±2°C at room temperature. On the top, the wet film thickness of the coating is 250μm, and then placed in a precision oven at 50±2℃ to dry for 3~4h to constant weight, take it out, and cool to room temperature to obtain the actual color block.
Example Embodiment
[0024] Example 2:
[0025] Weigh 0.05 g of PBK7, 5.61 g of PY138, 0.19 g of PG7, and 1000 g of CSC-A base material by weight. The production process is the same as in Example 1.
Example Embodiment
[0026] Example 3:
[0027] Weigh 0.05 g of PBK7, 5.65 g of PY138, 0.20 g of PG7, and 1005 g of CSC-A base by weight. The production process is the same as in Example 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap